Title: New Carboxylic Acid-Based Superplasticizer for High-Performance Concrete

Author(s): Y. C. Tseng, W. L. Wu, H. L. Huang, C. T. Wang, and K. C. Hsu

Publication: Symposium Paper

Volume: 195

Issue:

Appears on pages(s): 401-414

Keywords: cement; concrete; superplasticizer; workability

DOI: 10.14359/9925

Date: 7/1/2000

Abstract:
Superplasticizers are key components to enhance greatly the workability of concrete. A new carboxylic acid-based copolymer was synthesized and evaluated as a superplasticizer. This copolymer was prepared from methacrylic acid and 2-acrylamido-2-methylpropane sulfonic acid through free radical polymerization. The test results on cement pastes indicate that this copolymer could uniformly disperse the cement particles and improve the fluidity of the system. Compared to the commercially available naphthalene-based superplasticizer, the polymer requires less amount to achieve the same mini-slump value, and provides longer slump retention time. Thus the synthesized resin has a potential to become a superplasticizer. Finally, the workability and compressive strength of concrete with this new admixture were also tested, and compared with that of the commercial superplasticizers.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer