Title: Relationships Between Deterioration and Structural Performance: Three Case Studies

Author(s): R. A. Miller, B. M. Shahrooz, and A. E. Aktan

Publication: Symposium Paper

Volume: 154

Issue:

Appears on pages(s): 439-460

Keywords: beams (supports); bridges (structures); deterioration; models; nondestructive tests; performance; slabs; structural analysis; tests; Structural Research

DOI: 10.14359/990

Date: 5/1/1995

Abstract:
Examines the relationship between deterioration of concrete and the structural performance of bridge structures. Case 1: A 37-year-old, three-span concrete slab bridge was decommissioned due to heavy deterioration. Modal testing was used to detect the mos




  