International Concrete Abstracts Portal

  


Title: McAuto STRUDL RECON - A Reinforced Concrete Frame Design Software

Author(s): D. Dasgupta

Publication: Concrete International

Volume: 4

Issue: 11

Appears on pages(s): 37-42

Keywords: computer programs; computers; moments; reinforced concrete; structural analysis; structural design.

DOI:

Date: 11/1/1982

Abstract:
MCAUTO STRUDL is a structural analysis and design software that has been widely used by the engineering profession all over the world. Now a new reinforced concrete design feature called RECON has been added to it specifically aimed at common building frame applications. Its capabilities include moment- magnification, design of beams and columns in accordance with ACI 318-77 Building Code, and automated drafting of reinforcement details.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.