Title: Bond Creep And Shrinkage Effects In Reinfroced Concrete

Author(s): J. R. Shank

Publication: Journal Proceedings

Volume: 35

Issue: 11

Appears on pages(s): 81-92

Keywords: none

DOI: 10.14359/8480

Date: 11/1/1938

Abstract:
Bar splices were kept under constant load for more than 2 years during which time one bar of one test moved past the other 0.04 in. under a bond stress of 153 psi without losing the load. This was six times as treat as the average of five other tests. Stresses in the steel of similar specimens not under load showed that practically all of the stress due to shrinkage disappeared after 25 days. Before cracking occurred the stresses were only 40 percent of those calculated from data of unreinforced shrin kaqe.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer