Title: Testing Cast Stone
Author(s): ACI Committee 704
Publication: Journal Proceedings
Volume: 28
Issue: 9
Appears on pages(s): 33-36
Keywords: none
DOI: 10.14359/8227
Date: 9/1/1931
Abstract: Committee 704 reports on its test program concerning testing procedures and strength and density require-ments as covered by the Tentative Specification for Cast Stone (P3-A-29T) and recommends several changes in the specification.