Title: Hyperbolic Reinforced Concrete Towers
Author(s): Paul Rogers
Publication: Journal Proceedings
Volume: 58
Issue: 10
Appears on pages(s): 395-406
Keywords: none
DOI: 10.14359/7991
Date: 10/1/1961
Abstract: This paper describes the general features, operation, and economic advantages of the natural draft -type, hyper-bolically shaped, reinforced concrete cooling towers.