Title: Ultimate Strength Design Charts For Columns with Biaxial Bending

Author(s): Donald C. Weber

Publication: Journal Proceedings

Volume: 63

Issue: 11

Appears on pages(s): 1205-1230

Keywords: biaxial bending, column, design, short column, ultimate strength.

DOI: 10.14359/7667

Date: 11/1/1966

Abstract:
The problem of combined biaxzial bending and axial compression of short rectangular columns is discussed. A method of approximating the failure surface based on linear interpolation between the capacity for bending on the diagonal and the capacity for bending on a principal axis is proposed. Design charts for columns with equal bending resistance on both principal axes and examples to illustrate their use are included.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.