International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: HYDROGEN EVOLUTION FROM FERROPHOSPHOROUS AGGREGATE IN PORTLAND CEMENT CONCRETE . . . .

Author(s): T. G. Clendenning, B. Kellam, and C. Maclnnis

Publication: Journal Proceedings

Volume: 65

Issue: 12

Appears on pages(s): 1021-1028

Keywords:

DOI: 10.14359/7535

Date: 12/1/1968

Abstract:
Hydrogen evolution in a heavy concrete containing ferro-phosphorus aggregate was noted during construction of a biological shield for a nuclear generating station. While the reaction was of a self-limiting nature, the concrete would produce over 25 times its volume of hydrogen before the reaction ceased. The factors affecting the reaction and the possible mechanisms involved are discussed. Subsequent investigation has shown that a similar reaction occurs with ferrosilicon, another heavyweight slag, otherwise of poten-tial value in heavy concrete.




  

Edit Module Settings to define Page Content Reviewer