Effect of Nonlinear-Inelastic Connection Behavior on Precast Panelized S hearwalls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Nonlinear-Inelastic Connection Behavior on Precast Panelized S hearwalls

Author(s): C. Llorente, J. M. Becker, and J. M. Roesset

Publication: Symposium Paper

Volume: 63

Issue:

Appears on pages(s): 27-48

Keywords: concrete panels; connections; dynamic loads; earthquake' resistant structures; lateral pressure; loads (forces); mathemati-cal models; precast concrete; -- research; shearwalls; slippage.

DOI: 10.14359/6645

Date: 8/1/1980

Abstract:
This paper reports on preliminary results of research into the seismic response of large panel precast concrete construction typical of that used in the United States. Seismic . response is being modeled using finite element techniques and an explicit time step integration procedure. The seismic resisting elements of a crosswall system have been isolated to study the role the connection regions may have in seismic response. Results are presented that show the effects associated with rocking type motion and slpage in the horizontal connections of isolated crosswalls.




  