Title:
Use of Concrete Polymer Materials in the Transportation Industry
Author(s):
Jack J. Fontana
and John Bartholomew
Publication:
Symposium Paper
Volume:
69
Issue:
Appears on pages(s):
21-44
Keywords:
bridge decks; concrete construction; corrosion; deteri-oration;
durability; field tests; impregnating; maintenance;
patching; polymer concrete; portland cements; repairs; resurfac-ing;
strength; transportation.
DOI:
10.14359/6377
Date:
8/1/1981
Abstract:
Every segment of the transportation industry is experiencing maintenance problems with rapidly deteriorating portland cement concrete structures. The Federal Highway Administration, aware of such problems, has sponsored research and development work to find a rapid-setting durable composite that can be used to repair deteriorated concrete and/or to effectively reduce chloride and moisture penetration into concrete.