Title:
Polymer Concrete Overlays
Author(s):
F. Mendis
Publication:
Symposium Paper
Volume:
93
Issue:
Appears on pages(s):
525-562
Keywords:
abrasion resistance; aggregates; bridge decks;
epoxy resins; methyl methacrylate; polyester resins; polymer
concrete; resurfacing; screeds; skid resistance
DOI:
10.14359/6318
Date:
9/1/1986
Abstract:
Polymer concretes are finding increasing use as bridge deck overlays. They are impermeable, skid resistant, lightweight and develop strong bonds to well prepared bridge decks. The properties of the polymeric binders and aggregates used to form the polymer concrete are important to the success of the polymer concrete overlays. The binders should be strong and yet flexible and low modulus and the aggregates should behard and resistant to polishing and fracturing. Case histories where such overlays were used in major projects are described in detail together with the methods and equipment used in their application.