International Concrete Abstracts Portal

  


Title: FEM Pressure Estimation of Confined Expansive Concrete

Author(s): K. Yamada, T. Harada, K. Soeda and A. Watanabe

Publication: Symposium Paper

Volume: 179

Issue:

Appears on pages(s): 875-886

Keywords: confined concrete; expansive cement; finite element method

DOI: 10.14359/6077

Date: 6/1/1998

Abstract:
The pressure of expansive concrete under confinement was investigated by the finite element method, FEM. It was found that it was possible to estimate the pressure of expansive concrete by simple elastic calculation using FEM where the elastic modulus was assumed to be l-3 GPa, which was an order of magnitude lower than that of normal concrete. Experimental data giving the pressure of expansive concrete under confinement was successfully explained by the FEM calculation. It is demonstrated that FEM analysis is a useful tool to estimate the pressure of expansive concrete under various confinement conditions.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer