Title: 364.3R-09: Guide for Cementitious Repair Material Data Sheet
Author(s): ACI Committee 364
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 12
Keywords: data protocol; material properties; repair material; test methods.
DOI:
Date: 4/1/2009
Abstract: The purpose of this document is to provide a guide to the protocol for testing and reporting of data for cementitious repair materials. It does not address all of the issues associated with material selection. It is the responsibility of the user of this document to determine the suitability of the repair material before use.