Characterizing Continuous Curing and Compressive Piezoresistive Stress and Strain Behavior of Smart Cement Modified with Inorganic and Organic Additives and the Performances Predicted using Vipulanandan Models

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Characterizing Continuous Curing and Compressive Piezoresistive Stress and Strain Behavior of Smart Cement Modified with Inorganic and Organic Additives and the Performances Predicted using Vipulanandan Models

Author(s): C. Vipulanandan

Publication: Symposium Paper

Volume: 369

Issue:

Appears on pages(s): 114-130

Keywords: Smart cement, Electrical resistivity, Sodium meta silicate (SMS), Acetone formaldehyde sulfite (AFS), Curing, Compression, Piezoresistive Behavior, Vipulanandan Models.

DOI: 10.14359/51750726

Date: 5/1/2026

Abstract:
Recently highly sensing smart cements, for both oil well cements and Portland cements, have been developed. Based on the new electrical characterization method electrical resistivity was identified as the critical property of the cement to monitor during curing (changing from slurry to solid) and also in-service (solid). In this study 0.3% of sodium meta silicate (SMS), inorganic additive to reduce amount of cement in the cement slurry and a dispersant (acetone formaldehyde sulfite--AFS), organic additive to reduce the amount of water in the cement slurry were selected and used to modify the smart cement. With the addition of 0.3% SMS to the cement slurry with water-cement ratio of 0.4 the initial resistivity (immediately after mixing) reduced from 0.97 Ωm to 0.88 Ωm, about 9.3% reduction. The compressive strength after 28 days of curing reduced from 36.23 MPa to 34.68 MPa, a 4% reduction and the piezoresistive modulus increased by 166%. The piezoresistive strain at peak compressive stress reduced from 315% to 148%, a 53% reduction with the addition of 0.3% SMS. With the addition of 0.3% AFS to the cement slurry with water-to-cement ratio of 0.38 the initial resistivity reduced from 1.08 Ωm to 0.83 Ωm, about 23% reduction. The compressive strength after 28 days of curing increased from 30.1 MPa to 37.7 MPa, a 25% increase with the addition of 0.3% AFS) (clear indication from higher resistivity index (RI24) – higher chemical reactions) but the piezoresistive modulus decreased by 26%. The piezoresistive strain at peak compressive stress increased from 164% to 184%, a 12% increase with the addition of 0.3% AFS. The curing of smart cement with the additives were predicted using the Vipulanandan Curing Model. Vipulanandan stress- piezoresistive axial strain model predicted the compressive stress-piezoresistive strain relationships very well.

Related References:

1. Nelson, E.B., 1990. Well Cementing. Elsevier Science BV, Amsterdam, The Netherlands, 1990, pp. 3-10.

2. Calvert, D. G., Smith, D. K., 1990. API Oil Well Cementing Practices. Journal of Petroleum Technology, Volume 42, Issue 11, November, 1990.

3. Izon, D., Danenberger, E.P., and Mayes, M., 2007. Absence of fatalities in blowouts encouraging in MMS study of OCS incidents 1992-2006. Well Control Magazine, July/August 2007, pp. 86-90.

4. Davies, R. J., Almond, S., Ward, R. S., Jackson, R. B., Adams, C., Worrall, F., Whitehead, M. A. (2014). Oil and gas wells and their integrity: Implications for shale and unconventional resource exploitation. Marine and Petroleum Geology, Vol. 56, pp. 239-254.

5. API Specification 10A (2002), Specification for Cements and Materials for Well Cementing, 23rd Edition, American Petroleum Institute, Washington D.C.

6. Bao-guo H, and Jin-ping O., (2008). Humidity sensing property of cements with added carbon, New Carbon Materials, Vol. 23, pp. 382-384.

7. Mbaba, P.E. and Caballero, E.P. 1983. Field Application of an Additive Containing Sodium Metasilicate During Steam Stimulation. Proceeding-SPE Annual Technical Conference and Exhibition, San Francisco, California, 5-8 October, 1983.

8. Larrondo, L.E., Urness, C.M., and Milosz, G.M., 1985. Laboratory Evaluation of Sodium Hydroxide, Sodium Orthosilicate, and Sodium Metasilicate as Alkaline Flooding Agents for a Western Canada Reservoir. Proceeding- SPE Oilfield and Geothermal Chemistry Symposium, Phoenix, Arizona, 9-11 March, 1985.

9. U.S. Patent Number 10,481,143 Awarded on November 19, 2019 Chemo-Thermo-Piezoresistive highly Sensing Smart Cement with Integrated Real-Time Monitoring System Inventor: C. Vipulanandan - International Patent App. PCT/US2016/041905, 2016 ;(WO2017022460).

10. Vipulanandan, C. (2021) Smart Cement: Development, Testing, Modeling and Real-Time Monitoring, Taylor and Francis CRC Press, pp. 402.

11. Vipulanandan, C, Maddi, A.R. and Chandra Mohan (2024) Smart Piezoresistive Plasterof Paris for Real-time Monitoring of Curing and Compressive Stress Changes Quantified Using Vipulanandan Models, Journal of Material Performance and Engineering, Vol. 33, (17) pp. 9059-9069.

12. Vipulanandan, C., and Ali, K., (2018) Smart Cement Grouts for Repairing Damaged Piezoresistive Cement and the Performances Predicted Using Vipulanandan Models Journal of Civil Engineering Materials, American Society of Civil Engineers (ASCE), Vol. 30, No. 10, pp. 1-8, Article number 04018253.

13. Fuller, G., Souza, P., Ferreira, L., and Rouat, D. (2002). High-Strength Lightweight Blend Improves Deepwater Cementing, Oil & Gas Journal, Vol. 100, No.8, pp. 86-95.

14. Ramachandran, V.S., Feldman, R.F., Beaudoin, J.J. (1981), Concrete Science: Treatise On Current Research, Heyden and Son. Ltd., Philadelphia.

15. Plank, J. and Hirsch, C. (2007). Impact of zeta potential of early cement hydration phases on superplasticizer adsorption, Cement and Concrete Research 37, pp. 537–542.

16. Gretz, M. and Plank, J. (2010). Hybrid additives for construction applications, fabricated through layer-by- layer adsorption of polycondensate type superplasticizers on latex templates. J, Colloids and Surfaces A: Physicochem. Eng. Aspects Vol. 366. pp. 38-44.

17. Amani, N., Vipulanandan, C. and Plank, J. (2020), Monitoring the hydration and strength development in piezoresistive cement admixture with superplasticizer and retarder additives, Journal of Petroleum Science and Engineering, 195 (2020) 107601, pp.1-9.

18. Kong, H., Bike, S., Li, V. (2006), Effects of a strong polyelectrolyte on the rheological properties of concentrated cementitious suspensions, Cement and Concrete Research Vol. 36, pp. 851– 857.

19. ASTM C191 (2019) Test Method for Time of Setting of Hydraulic Cement by Vicat Needle, ASTM International, West Conshohocken, PA, USA.