One-Way Shear Design for Transverse Bar-Free Ultra-High-Performance Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: One-Way Shear Design for Transverse Bar-Free Ultra-High-Performance Concrete Members

Author(s): Abdulrahman Salah and Dimitrios Kalliontzis

Publication: Structural Journal

Volume: 123

Issue: 2

Appears on pages(s): 311-324

Keywords: ACI 318; fiber alignment; shear design; size effects; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51749307

Date: 3/1/2026

Abstract:
This paper presents a design model for the one-way shear of ultra-high-performance concrete (UHPC) beams without transverse reinforcement. The model unifies the shear design of UHPC with the ACI 318 shear design approach for conventional concrete. Hence, the proposed model accounts for the longitudinal reinforcement ratio and the axial load effects, while the tensile strength of UHPC replaces the concrete compressive strength term. The effects of fiber type, fiber alignment, beam shape, and beam size are incorporated through dimensionless parameters, with their values calibrated using UHPC beam and panel shear data sets. The proposed shear model was evaluated using a database of 137 UHPC nonprestressed and prestressed rectangular and I-shaped beam shear tests performed in the United States and elsewhere.

Related References:

1. Ridha, M. M. S.; Al-Shaarbaf, I. A. S.; and Sarsam, K. F., “Experimental Study on Shear Resistance of Reactive Powder Concrete Beams Without Stirrups,” Mechanics of Advanced Materials and Structures, V. 27, No. 12, 2020, pp. 1006-1018. doi: 10.1080/15376494.2018.1504258

2. Voo, Y. L.; Foster, S. J.; and Gilbert, R. I., “Shear Strength of Fiber Reinforced Reactive Powder Concrete Prestressed Girders without Stirrups,” Journal of Advanced Concrete Technology, V. 4, No. 1, 2006, pp. 123-132. doi: 10.3151/jact.4.123

3. Huang, Y., and Yao, G., “Shear Strength of Ultra-High-Performance Concrete Beams without Stirrups—A Review Based on a Database,” Buildings, V. 14, No. 5, May 2024, Article No. 1212. doi: 10.3390/buildings14051212

4. Kodsy, A., and Morcous, G., “Shear Strength of Ultra-High-Performance Concrete (UHPC) Beams without Transverse Reinforcement: Prediction Models and Test Data,” Materials, V. 15, No. 14, July 2022, Article No. 4794. doi: 10.3390/ma15144794

5. Metje, K., and Leutbecher, T., “Verification of the Shear Resistance of UHPFRC Beams – Design Method for the German DAfStb Guideline and Database Evaluation,” Engineering Structures, V. 277, Feb. 2023, Article No. 115439. doi: 10.1016/j.engstruct.2022.115439

6. Hussein, L., and Amleh, L., “Shear Behavior of UHPFRC Beams Without Stirrups,” Proceedings of the 10th fib International PhD Symposium in Civil Engineering, J. Bastien, N. Rouleau, M. Fiset, and M. Thomassin, eds., Université Laval, Québec, QC, Canada, July 2014, pp. 437-442.

7. Yang, I.-H.; Joh, C.; and Kim, B.-S., “Shear Behaviour of Ultra-High-Performance Fibre-Reinforced Concrete Beams Without Stirrups,” Magazine of Concrete Research, V. 64, No. 11, Nov. 2012, pp. 979-993. doi: 10.1680/macr.11.00153

8. El-Helou, R. G., and Graybeal, B. A., “Shear Behavior of Ultrahigh-Performance Concrete Pretensioned Bridge Girders,” Journal of Structural Engineering, ASCE, V. 148, No. 4, Apr. 2022, p. 04022017. doi: 10.1061/(ASCE)ST.1943-541X.0003279

9. Yavas, A., and Goker, C. O., “Impact of Reinforcement Ratio on Shear Behavior of I-Shaped UHPC Beams with and without Fiber Shear Reinforcement,” Materials, V. 13, No. 7, Apr. 2020, Article No. 1525. doi: 10.3390/ma13071525

10. Vecchio, F. J., and Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

11. El-Helou, R. G., and Graybeal, B. A., “Shear Design of Strain-Hardening Fiber-Reinforced Concrete Beams,” Journal of Structural Engineering, ASCE, V. 149, No. 2, Feb. 2023, p. 04022234. doi: 10.1061/JSENDH.STENG-11065

12. Foster, S. J., and Bentz, E., “Design of UHPC Prestressed Girders for Shear,” Structural Concrete, V. 25, No. 2, Apr. 2024, pp. 780-795. doi: 10.1002/suco.202300738

13. Diab, A., and Ferche, A., “Shear Strength Model for UHPC Members Incorporating Fiber Orientation and Cross-Sectional Shape Effects: Model Formulation and Database Evaluation,” Engineering Structures, V. 327, Mar. 2025, Article No. 119654. doi: 10.1016/j.engstruct.2025.119654

14. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 227 pp.

15. DAfStb, “DAfStb-Richtlinie: Stahlfaserbeton,” German Committee for Structural Concrete, Berlin, Germany, 2021, 52 pp.

16. Diab, A., and Ferche, A. C., “Modeling the Response of UHPFRC Shear-Critical Beams: Integrating Nonlinear Finite Element Analysis and Machine Learning,” SSRN, 2024, 40 pp.

17. Shahin, N.; Salah, A.; and Kalliontzis, D., “Softened Membrane Model for Shear of Ultra-High-Performance Concrete (SMM-UHPC),” Engineering Structures, V. 308, June 2024, Article No. 117956. doi: 10.1016/j.engstruct.2024.117956

18. Zhang, Z.; Vecchio, F. J.; Bentz, E. C.; and Foster, S. J., “Modeling of Ultra-High-Performance Fiber-Reinforced Concrete in Shear,” ACI Structural Journal, V. 119, No. 1, Jan. 2022, pp. 295-305.

19. Salah, A.; Kalliontzis, D.; Lawler, J. S.; and Wagner, E. I., “Shear Behavior of Reinforcing Bar-Free Ultra-High-Performance Concrete Considering Axial Load Effects and Fiber Alignment,” ACI Structural Journal, V. 122, No. 2, Mar. 2025, pp. 215-230.

20. Salah, A., and Kalliontzis, D., “Size Effects in UHPC Shear Considering Depth, Width, and Fiber Alignment,” Engineering Structures, V. 338, Sept. 2025, Article No. 120544.

21. AASHTO, “Guide Specifications for Structural Design with Ultra-High Performance Concrete,” first edition, American Association of State Highway and Transportation Officials, Washington, DC, 2024, 97 pp.

22. Tadros, M.; Lawler, J.; Abo El-Khier, M.; Gee, D.; Kurt, A.; Lucier, G.; and Wagner, E., “Implementation of Ultra-High-Performance Concrete in Long-Span Precast Pretensioned Elements for Concrete Buildings and Bridges, Phase II Report,” Precast/Prestressed Concrete Institute, Chicago, IL, 2021, 753 pp.

23. Ross, B.; Tarawneh, A.; Naser, M. Z.; Ferche, A. C.; Diab, A.; and Craig, D., “Comparison of Recent Shear Capacity Models with Experimental and Simulation Databases of Prestressed Ultra-High-Performance Concrete Beams,” PCI Journal, V. 69, No. 6, Nov.-Dec. 2024, pp. 37-57. doi: 10.15554/pcij69.6-01

24. Hsu, T. T. C., and Mo, Y. L., Unified Theory of Concrete Structures, John Wiley & Sons, Ltd., Chichester, UK, 2010, 521 pp.

25. Hsu, T. T. C.; Belarbi, A.; and Pang, X., “A Universal Panel Tester,” Journal of Testing and Evaluation, V. 23, No. 1, 1995, pp. 41-49. doi: 10.1520/JTE10397J

26. Li, V. C.; Lin, Z.; and Matsumoto, T., “Influence of Fiber Bridging on Structural Size-Effect,” International Journal of Solids and Structures, V. 35, No. 31-32, Nov. 1998, pp. 4223-4238. doi: 10.1016/S0020-7683(97)00311-9

27. Wille, K., and Parra-Montesinos, G. J., “Effect of Beam Size, Casting Method, and Support Conditions on Flexural Behavior of Ultra-High-Performance Fiber-Reinforced Concrete,” ACI Materials Journal, V. 109, No. 3, May-June 2012, pp. 379-388.

28. Crane, C. K., “Shear and Shear Friction of Ultra-High Performance Concrete Bridge Girders,” PhD dissertation, Georgia Institute of Technology, Atlanta, GA, 2010, 348 pp.

29. Yoo, D.-Y.; Banthia, N.; Kang, S.-T.; and Yoon, Y.-S., “Size Effect in Ultra-High-Performance Concrete Beams,” Engineering Fracture Mechanics, V. 157, May 2016, pp. 86-106. doi: 10.1016/j.engfracmech.2016.02.009

30. Baby, F.; Marchand, P.; and Toutlemonde, F., “Shear Behavior of Ultrahigh Performance Fiber-Reinforced Concrete Beams. I: Experimental Investigation,” Journal of Structural Engineering, ASCE, V. 140, No. 5, May 2014, p. 04013111. doi: 10.1061/(ASCE)ST.1943-541X.0000907

31. Boulekbache, B.; Hamrat, M.; Chemrouk, M.; and Amziane, S., “Flowability of Fibre-Reinforced Concrete and Its Effect on the Mechanical Properties of the Material,” Construction and Building Materials, V. 24, No. 9, Sept. 2010, pp. 1664-1671. doi: 10.1016/j.conbuildmat.2010.02.025

32. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

33. Belarbi, A.; Kuchma, D. A.; and Sanders, D. H., “Proposals for New One-Way Shear Equations for the 318 Building Code,” Concrete International, V. 39, No. 9, Sept. 2017, pp. 29-32.

34. ACI Committee 318, “Building Code for Structural Concrete—Code Requirements and Commentary (ACI CODE-318-25),” American Concrete Institute, Farmington Hills, MI, 2025, 702 pp.

35. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

36. Frosch, R. J.; Yu, Q.; Cusatis, G.; and Bažant, Z. P., “A Unified Approach to Shear Design,” Concrete International, V. 39, No. 9, Sept. 2017, pp. 47-52.

37. Kuchma, D. A.; Wei, S.; Sanders, D. H.; Belarbi, A.; and Novak, L. C., “Development of the One-Way Shear Design Provisions of ACI 318-19 for Reinforced Concrete,” ACI Structural Journal, V. 116, No. 4, July 2019, pp. 285-295.

38. Pujol, S.; Ospina, C. E.; and Kerby, C., “A Lower Bound to the Shear Strength of RC Beams and One-Way Members without Shear Reinforcement,” Concrete International, V. 46, No. 6, June 2024, pp. 50-55.

39. RILEM Technical Committee 162-TDF, “Test and Design Methods for Steel Fibre Reinforced Concrete - Recommendations: σ-ε-Design Method,” Materials and Structures, V. 33, No. 2, Mar. 2000, pp. 75-81.

40. fib, “fib Model Code for Concrete Structures 2010,” International Federation for Structural Concrete, Lausanne, Switzerland, 2013, 434 pp.

41. NF P 18-710:2016, “National Addition to Eurocode 2—Design of Concrete Structures: Specific Rules for Ultra-High Performance Fibre-Reinforced Concrete (UHPFRC),” Association Française de Normalisation (AFNOR), Paris, France, 2016, 136 pp.

42. Buckingham, E., “On Physically Similar Systems; Illustrations of the Use of Dimensional Equations,” Physical Review, V. 4, No. 4, Oct. 1914, pp. 345-376. doi: 10.1103/PhysRev.4.345

43. Huang, H.; Su, A.; Gao, X.; and Yang, Y., “Influence of Formwork Wall Effect on Fiber Orientation of UHPC with Two Casting Methods,” Construction and Building Materials, V. 215, Aug. 2019, pp. 310-320. doi: 10.1016/j.conbuildmat.2019.04.200

44. The MathWorks, Inc., “MATLAB,” Natick, MA, 2024.

45. Wu, X., and Han, S.-M., “First Diagonal Cracking and Ultimate Shear of I-Shaped Reinforced Girders of Ultra High Performance Fiber Reinforced Concrete without Stirrup,” International Journal of Concrete Structures and Materials, V. 3, No. 1, 2009, pp. 47-56. doi: 10.4334/IJCSM.2009.3.1.047

46. Ţibea, C., and Bompa, D. V., “Ultimate Shear Response of Ultra-High-Performance Steel Fibre-Reinforced Concrete Elements,” Archives of Civil and Mechanical Engineering, V. 20, No. 2, June 2020, Article No. 49. doi: 10.1007/s43452-020-00051-z

47. AASHTO T 397-22, “Standard Method of Test for Uniaxial Tensile Response of Ultra-High Performance Concrete,” American Association of State Highway and Transportation Officials, Washington, DC, 2022, 49 pp.

48. Hung, C.-C.; El-Tawil, S.; and Chao, S.-H., “A Review of Developments and Challenges for UHPC in Structural Engineering: Behavior, Analysis, and Design,” Journal of Structural Engineering, ASCE, V. 147, No. 9, Sept. 2021, p. 03121001. doi: 10.1061/(ASCE)ST.1943-541X.0003073

49. Tarawneh, A.; Amirah, H.; Alawadi, R.; and Diab, A., “Shear Resistance of UHPC Girders: Experimental Database Evaluation of the FHWA-HRT-23-077,” Structures, V. 70, Dec. 2024, Article No. 107895. doi: 10.1016/j.istruc.2024.107895


ALSO AVAILABLE IN:

Electronic Structural Journal