Evaluating Fresh and Hardened Properties of Self-Consolidating Concrete Containing Different Supplementary Cementitious Materials/Fillers

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluating Fresh and Hardened Properties of Self-Consolidating Concrete Containing Different Supplementary Cementitious Materials/Fillers

Author(s): Morcous

Publication: Web Session

Volume: ws_S25_Morcous.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
Fresh, early-age, and hardened concrete properties were evaluated in a laboratory investigation of forty SCC mixtures proportioned using: two types of coarse aggregate—crushed limestone and natural gravel; three nominal maximum sizes of aggregate (NMSA)—¾, ½, and 3/8 in.; three SCMs and one filler—25% Class F fly ash, 25% Class C fly ash, 30% ground granulated blast-furnace slag (GGBFS), and 20% Class F fly ash +15% limestone powder (LSP); and two levels of slump flow—low (22–26 in.) and high (26–30 in.). All SCC mixtures were air entrained and contained Portland cement Type I/II. The laboratory tests were conducted according to AASHTO or ASTM methods. Measured properties of SCC mixtures were compared to predicted values using existing prediction models.




  