Low-Portland Cement Concrete Mixtures Made with Ultrafine Granulated Blast Furnace Slag and Medium-Grade Metakaolin

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Low-Portland Cement Concrete Mixtures Made with Ultrafine Granulated Blast Furnace Slag and Medium-Grade Metakaolin

Author(s): Saeid Ghasemalizadeh

Publication: Web Session

Volume: ws_S25_SaeidGhasemalizadeh.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/30/2025

Abstract:
This study investigated enhancing effects of ultrafine slag (UFS) and its combination with a locally-available medium-grade metakaolin (MK) in developing low-Portland cement (PC) mixtures. UFS was obtained by ultrafine grinding of slag and then blended with MK in different ratios to replace 50 wt% of PC in mortar and concrete samples. Based on the results, small amounts of UFS combined with MK could replace 50 wt% of PC and obtain a similar 3-d compressive strength and higher 28-d strength compared to that achieved with 100 wt% PC. According to the microstructural analyses, the strength enhancement was mainly attributed to the increased reactivity of UFS compared to slag, which promoted the formation of calcium-aluminium-silicate-hydrate and hemi- and monocarboaluminates. The preliminary environmental impact analysis showed that the concrete with the UFS-MK blend could have a lower greenhouse gas emissions per unit strength compared to that made with the slag-MK blend.




  