Title: ACI PRC-524.1-24: Swimming Pool Plastering—TechNote

Author(s): C0052400

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 3

Keywords:

DOI:

Date: 12/19/2024

Abstract:
Like traditional plaster, pool plaster is intended to be a nonstructural finish; however, its intended application is for aqueous environments. The materials and methods for plastering swimming interior finishes differ from traditional plastering. This TechNote outlines these basic differences. Keywords: calcium chloride; cementitious; hand-troweled materials; plastering; substrate; swimming pools.




  