Title:
Expanding the Pour Season for Bridge Deck Overlays with Latex Modified Concrete
Author(s):
Curt Costello
Publication:
Web Session
Volume:
ws_S24_CurtCostello.pdf
Issue:
Appears on pages(s):
Keywords:
DOI:
Date:
3/24/2024
Abstract:
Recent research expands the understanding of Latex Modified Concrete (LMC) performance under low temperature cure conditions. Learn how the results support the extension of the LMC installation season into late fall and early spring, providing greater flexibility for DOTs and contractors focused on improving U.S. infrastructure.