Title:
Utilization of Electric Arc Furnace Slag for CO2 Storage in Mortar using Pressurized CO2 Curing Condition
Author(s):
Indong Jang, Namkon Lee, Hoon Moon, Gijoon Park, Gumsung Ryu, Jungjun Park
Publication:
Symposium Paper
Volume:
362
Issue:
Appears on pages(s):
444-452
Keywords:
carbonation, pressurized CO2 curing, steel slag
DOI:
10.14359/51740902
Date:
6/11/2024
Abstract:
Electric arc furnace slag is a byproduct generated in the steel industry, which can be categorized into oxidizing slag (electric arc furnace oxidizing slag, EOS) and reducing slag (electric arc furnace reducing slag, ERS) depending on the manufacturing process. These slags contain ions such as Ca, Si, and Mg in unstable states, allowing them to form minerals through reactions with CO2. In this study, we investigated the carbonation efficiency of cement mortar incorporating these slags as supplementary mineral admixture and aggregates, under varying CO2 curing conditions. CO2 curing was conducted under a 99% concentration CO2 at a pressure of 10 bar. The curing temperatures were adjusted to 20℃ [68°F], 60℃ [140°F], and 90℃ [194°F], and compressive strength and carbonation depth were measured according to the slag substitution rate. Cement mortar with slag shows higher in both compressive strength and carbonation depth.
Related References:
1.Pacheco Torgal, F., S. Miraldo, J.A. Labrincha, and J. De Brito, An overview on concrete carbonation in the contextof eco-efficient construction: Evaluation, use of SCMs and/or RAC. Construction and Building Materials, 2012. 36: p. 141-150.
2.Galan, I., C. Andrade, P. Mora, and M.A. Sanjuan, Sequestration of CO2 by concrete carbonation. Environmentalscience & technology, 2010. 44(8): p. 3181-3186.
3.Fernandez Bertos, M., S.J. Simons, C.D. Hills, and P.J. Carey, A review of accelerated carbonation technology in thetreatment of cement-based materials and sequestration of CO2. J Hazard Mater, 2004. 112(3): p. 193-205.
4.Sanjuán, M.Á., E. Estévez, C. Argiz, and D.d. Barrio, Effect of curing time on granulated blast-furnace slag cementmortars carbonation. Cement and Concrete Composites, 2018. 90: p. 257-265.
5.Mehta, P.K. and P.J. Monteiro, Concrete: microstructure, properties, and materials. 2014: McGraw-Hill Education.
6.Li, X. and T.-C. Ling, Instant CO2 curing for dry-mix pressed cement pastes: Consideration of CO2 concentrationscoupled with further water curing. Journal of CO2 Utilization, 2020. 38: p. 348-354.
7.Wang, L., et al., Biochar as green additives in cement-based composites with carbon dioxide curing. Journal of CleanerProduction, 2020. 258: p. 120678.
8.Zhang, D. and Y. Shao, Surface scaling of CO2-cured concrete exposed to freeze-thaw cycles. Journal of CO2Utilization, 2018. 27: p. 137-144.
9.Zhang, D., V.C. Li, and B.R. Ellis, Ettringite-related dimensional stability of CO2-cured Portland cement mortars.ACS Sustainable Chemistry & Engineering, 2019. 7(19): p. 16310-16319.
10.Rostami, V., Y. Shao, and A.J. Boyd, Durability of concrete pipes subjected to combined steam and carbonation curing.Construction and Building Materials, 2011. 25(8): p. 3345-3355.
11.Zhang, S., Z. Ghouleh, and Y. Shao, Effect of carbonation curing on efflorescence formation in concrete paver blocks. Journal of Materials in Civil Engineering, 2020. 32(6): p. 04020127.
12.Zhang, D. and Y. Shao, Effect of early carbonation curing on chloride penetration and weathering carbonation inconcrete. Construction and Building Materials, 2016. 123: p. 516-526.
13.Zhang, D. and Y. Shao, Early age carbonation curing for precast reinforced concretes. Construction and BuildingMaterials, 2016. 113: p. 134-143.
14.Shao, Y., M.S. Mirza, and X. Wu, CO2 sequestration using calcium-silicate concrete. Canadian Journal of CivilEngineering, 2006. 33(6): p. 776-784.
15.San-José, J.T., I. Vegas, I. Arribas, and I. Marcos, The performance of steel-making slag concretes in the hardenedstate. Materials & Design, 2014. 60: p. 612-619.
16.Kim, J. and G. Azimi, The CO2 sequestration by supercritical carbonation of electric arc furnace slag. Journal of CO2 Utilization, 2021. 52: p. 101667.
17.Ukwattage, N.L., P.G. Ranjith, and X. Li, Steel-making slag for mineral sequestration of carbon dioxide by acceleratedcarbonation. Measurement, 2017. 97: p. 15-22.