Rheology of Stabilized Earth-Based Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rheology of Stabilized Earth-Based Paste

Author(s): Mojtaba Kohandelnia and Ammar Yahia

Publication: Symposium Paper

Volume: 362

Issue:

Appears on pages(s): 108-126

Keywords: sustainable building; self-consolidating earth concrete; clay; rheology; supplementary cementitious materials

DOI: 10.14359/51740878

Date: 6/5/2024

Abstract:
Earthen construction techniques in sustainable building can offer numerous advantages. However, it comes with certain limitations, with the most notable one being the labor-intensive and time-consuming nature of the construction process. To address this challenge, self-consolidating earth concrete (SCEC) emerges as a promising solution, particularly when dealing with the presence of fine clay and silt particles, as it can help attain the desired rheological properties more efficiently. In this study, supplementary cementitious materials (SCMs) such as cement, metakaolin, and limestone filler have been used as stabilizers to evaluate their impact on the workability and rheology of earth-based mixtures. A high-range water-reducing polycarboxylate ether (PCE), either with or without the initial incorporation of sodium hexametaphosphate, was applied to various clay compositions. The presence of finer clay particles required a higher dosage of admixture to achieve the desired workability, resulting in elevated yield stress and plastic viscosity values.

Related References:

1. E.M. Gartner, D.E. MacPhee, A physico-chemical basis for novel cementitious binders, Cem. Concr. Res. 41 (2011) 736–749. doi: 10.1016/J.CEMCONRES.2011.03.006

2. S. Mousavinezhad, G.J. Gonzales, W.K. Toledo, J.M. Garcia, C.M. Newtson, S. Allena, A Comprehensive Study on Non-Proprietary Ultra-High-Performance Concrete Containing Supplementary Cementitious Materials, Materials (Basel). 16 (2023). doi: 10.3390/ma16072622

3. S. Mousavinezhad, J.M. Garcia, W.K. Toledo, C.M. Newtson, A Locally Available Natural Pozzolan as a Supplementary Cementitious Material in Portland Cement Concrete, Buildings. 13 (2023). doi: 10.3390/buildings13092364

4. C. Newtson, B. Weldon, J. Garcia, S. Mousavinezhad, W. Toledo, Durability of Concrete Produced with Alternative Supplementary Cementitious Material, 2021. https://repository.lsu.edu/transet_pubs/109.

5. H. Guillaud, H. Houben, Earth Construction: A Comprehensive Guide, Intermediate Technology Publications, 1994.

6. H. Van Damme, H. Houben, Earth concrete. Stabilization revisited, Cem. Concr. Res. 114 (2018) 90–102. doi: 10.1016/J.CEMCONRES.2017.02.035.

7. R. Bahar, M. Benazzoug, S. Kenai, Performance of compacted cement-stabilised soil, Cem. Concr. Compos. 26 (2004) 811–820. doi: 10.1016/j.cemconcomp.2004.01.003

8. M. Hall, Y. Djerbib, Rammed earth sample production: Context, recommendations and consistency, Constr. Build. Mater. 18 (2004) 281–286.

doi: 10.1016/j.conbuildmat.2003.11.001

9. M. Kohandelnia, M. Hosseinpoor, A. Yahia, R. Belarbi, Hygrothermal and microstructural characterization of self-consolidating earth concrete (SCEC), J. Build. Eng. 69 (2023) 106287. doi: 10.1016/J.JOBE.2023.106287

10. C.M. Ouellet-Plamondon, G. Habert, Self-Compacted Clay based Concrete (SCCC): Proof-ofconcept, J. Clean. Prod. 117 (2016) 160–168. doi: 10.1016/j.jclepro.2015.12.048

11. M. Kohandelnia, Development of Self-Consolidating Earth Concrete (SCEC) with Improved Multifunctional Performance for Green Construction, Université de Sherbrooke, 2022. http://hdl.handle.net/11143/20243.

12. M. Kohandelnia, M. Hosseinpoor, A. Yahia, R. Belarbi, Introduction of self-consolidating earth concrete (SCEC) and investigation on the influencing parameters using taguchi method, in: First Int. RILEM Conf. Earthen Constr. - Fundam. Appl. a Circ. Econ., Paris, France, 2022.

13. M. Kohandelnia, M. Hosseinpoor, A. Yahia, R. Belarbi, A new approach for proportioning self-consolidating earth paste (SCEP) using the Taguchi method, Constr. Build. Mater. 347 (2022) 128579. doi: 10.1016/J.CONBUILDMAT.2022.128579

14. P. Walker, R. Keable, J. Martin, V. Maniatidis, Rammed earth: design and construction guidelines, IHS BRE, 2005.

15. S. Guiheneuf, Formulation et renforts de blocs en matériau terre pour une utilisation structurelle, INSA de Rennes, 2020. https://tel.archives-ouvertes.fr/tel-03194559.

16. M. Kohandelnia, M. Hosseinpoor, A. Yahia, R. Belarbi, Multiscale investigation of selfconsolidating earthen materials using a novel concrete-equivalent mortar approach, Constr. Build. Mater. 370 (2023) 130700. doi: 10.1016/J.CONBUILDMAT.2023.130700

17. A.W. Skempton, The Colloidal activity of clays, in: 3rd Int. Conf. Soil Mech. Found. Eng., London, 1953: pp. 47–61.

18. O.-L. Tang, Q.-M. Jiang, Stability Analysis of Slope under Different Soil Nailing Parameters Based on the GeoStudio, Int. J. Geohazards Environ. 1 (2015) 88–92. doi: 10.15273/ijge.2015.02.010

19. J.J. Chen, B.H. Li, P.L. Ng, A.K.H. Kwan, Adding granite polishing waste as sand replacement to improve packing density, rheology, strength and impermeability of mortar, Powder Technol. 364 (2020) 404–415.

20. F. Andreola, E. Castellini, J.M.F. Ferreira, S. Olhero, M. Romagnoli, Effect of sodium hexametaphosphate and ageing on the rheological behaviour of kaolin dispersions, Appl. Clay Sci. 31 (2006) 56–64. doi: 10.1016/j.clay.2005.08.004

21. F. Andreola, E. Castellini, G. Lusvardi, L. Menabue, M. Romagnoli, Release of ions from kaolinite dispersed in deflocculant solutions, Appl. Clay Sci. 36 (2007) 271–278. doi: 10.1016/j.clay.2006.10.002

22. E. Castellini, C. Berthold, D. Malferrari, F. Bernini, Sodium hexametaphosphate interaction with 2:1 clay minerals illite and montmorillonite, Appl. Clay Sci. 83–84 (2013) 162–170. doi: 10.1016/j.clay.2013.08.031

23. J.L. Amorós, V. Beltrán, V. Sanz, J.C. Jarque, Electrokinetic and rheological properties of highly concentrated kaolin dispersions: Influence of particle volume fraction and dispersant concentration, Appl. Clay Sci. 49 (2010) 33–43. doi: 10.1016/j.clay.2010.03.020

24. F. Andreola, M. Romagnoli, E. Castellini, G. Lusvardi, L. Menabue, Role of the surface treatment in the deflocculation of kaolinite, J. Am. Ceram. Soc. 89 (2006) 1107–1109. doi: 10.1111/j.1551-2916.2005.00814.x

25. G. Minke, Building With Earth: Design and Technology of a Sustainable Architecture, Birkhäuser Basel, Switzerland, 2006.

26. A.M. Matos, H. Varum, Self-Compacting Earth-Based Composites: Mixture Design and Multi-Performance Characterisation, Buildings. 12 (2022).

doi: 10.3390/buildings12050612

27. A. Mostafa, A. Yahia, New approach to assess build-up of cement-based suspensions, Cem. Concr. Res. (2016) 174–182. doi: doi: 10.1016/j. cemconres.2016.03.005

28. M.A. Moeini, M. Hosseinpoor, A. Yahia, Effectiveness of the rheometric methods to evaluate the build-up of cementitious mortars used for 3D printing, Constr. Build. Mater. 257 (2020) 119551. doi: 10.1016/J.CONBUILDMAT.2020.119551

29. M.A. Moeini, M. Hosseinpoor, A. Yahia, Yield stress of fine cement-based mortars: Challenges and potentials with rotational and compressional testing methods, Constr. Build. Mater. 314 (2022).

30. A. Perrot, D. Rangeard, A. Pierre, Structural built-up of cement-based materials used for 3D printing extrusion techniques, Mater. Struct. 49 (2016) 1213–1220.

31. Y. Qian, G. De Schutter, Enhancing thixotropy of fresh cement pastes with nanoclay in presence of polycarboxylate ether superplasticizer (PCE), Cem. Concr. Res. 111 (2018) 15–22. doi: 10.1016/J.CEMCONRES.2018.06.013

32. Y. Zhang, Y. Zhang, W. She, L. Yang, G. Liu, Y. Yang, Rheological and harden properties of the high-thixotropy 3D printing concrete, Constr. Build. Mater. 201 (2019) 278–285. doi: 10.1016/J.CONBUILDMAT.2018.12.061

33. R. Ferron, A. Gregori, Z. Sun, S.P. Shah, Rheological method to evaluate structural buildup in self-consolidating concrete cement pastes, ACI Mater. J. 104 (2007) 242–250.

34. A. Kaleta-Jurowska, S. Grzeszczyk, M. Dziubiński, Application of multiple step change in shear rate model for determination of thixotropic behaviour of cement pastes, J. Build. Eng. 32 (2020). doi: doi: 10.1016/j.jobe.2020.101494

35. O. H.Wallevik, D. Feys, J.E. Wallevik, K.H. Khayat, Avoiding inaccurate interpretations of rheological measurements for cement-based materials, Cem. Concr. Res. 78 (2015) 100–109. doi: doi: 10.1016/j.cemconres.2015.05.003

36. D. Feys, K.H. Khayat, Particle migration during concrete rheometry: How bad is it?, Mater. Struct. 50 (2017). doi: doi: 10.1617/s11527-016-0992-4

37. J. Mewis, N.J. Wagner, Colloidal Suspension Rheology, Cambridge University Press, Cambridge, 2011.

38. M. Kohandelnia, M. Hosseinpoor, A. Yahia, R. Belarbi, New insight on rheology of selfconsolidating earth concrete (SCEC), Powder Technol. 424 (2023) 118561. doi: 10.1016/J.POWTEC.2023.118561

39. ASTM C494, Standard Specification for Chemical Admixtures for Concrete, ASTM Stand. (2017).

40. ASTM D4318 − 17, Standard Test Methods for Liquid Limit, Plastic Limit, and Plasticity Index of Soils, ASTM Stand. (2017).

41. ASTM C305-20, Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency, ASTM Stand. (2020) 1–3. doi: 10.1520/C0305-20.2

42. N. Roussel, C. Stefani, R. Leroy, From mini-cone test to Abrams cone test: Measurement of cement-based materials yield stress using slump tests, Cem. Concr. Res. 35 (2005) 817–822. doi: 10.1016/j.cemconres.2004.07.032

43. M.S. Phadke, Quality Engineering using Robust Design, Prentice Hall, New Jersey, 1989.

44. P. Dhemla, P. Somani, B.L. Swami, A. Gaur, Optimizing the design of sintered fly ash light weight concrete by Taguchi and ANOVA analysis, Mater. Today Proc. (2022). doi: 10.1016/J.MATPR.2022.03.573

45. J. Esmaeili, K. Andalibi, O. Gencel, Mechanical characteristics of experimental multi-scale steel fiber reinforced polymer concrete and optimization by Taguchi methods, Constr. Build. Mater. 313 (2021) 125500. doi: 10.1016/J.CONBUILDMAT.2021.125500

46. R.K. Roy, A Primer on the Taguchi Method, Competitive Manufacturing Series, 1990.

47. N. Roussel, P. Coussot, “Fifty-cent rheometer” for yield stress measurements: From slump to spreading flow, J. Rheol. (N. Y. N. Y). 49 (2005) 705–718. doi: doi: 10.1122/1.1879041