Assessment of the Flexural Bond Stresses of New Generation GFRP Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessment of the Flexural Bond Stresses of New Generation GFRP Bars

Author(s): Jesús D. Ortiz, Zahid Hussain, Seyed-Arman Hosseini, Brahim Benmokrane and Antonio Nanni

Publication: Symposium Paper

Volume: 360

Issue:

Appears on pages(s): 318-329

Keywords: bond failure, bond stresses, development length, GFRP rebars, rebar slippage.

DOI: 10.14359/51740633

Date: 3/1/2024

Abstract:
As a result of the limited data available when the current ACI 440.11-22 development length equation was developed, certain parameters were disregarded. Additionally, the equation was based on bars that are no longer in use today, and significant advancements have been made in FRP material properties and production methods since its calibration. Conflicting research findings have led to differing perspectives on its reliability, with some suggesting it yields overly conservative results, while others argue it may overestimate bond strength. To address this concern, an experimental study was conducted to assess the bond stresses between GFRP bars and conventional concrete in under-reinforced concrete beams. The beams were reinforced using a single M16 (No.5) Glass/Vinyl-ester FRP sand-coated bar. Three different lap splice lengths (i.e., 40-, 60-, and 80-times bar diameter) were selected based on available literature. The results indicate that the bond is primarily governed by surface friction, with negligible impact from relative slippage. The lap-spliced specimens exhibited slippage failure but exceeded design moments based on ACI provisions, indicating efficient performance. Stiffness remained comparable to that of the un-spliced beam, suggesting intact bond capacity despite some slippage. Average bond stress calculations closely aligned with ACI maximum bond stress values. Overall, the study offers valuable insights into GFRP bar behavior and bond capacity.

Related References:

1. Nanni, A., de Luca, A., and Jawaheri Zadeh, H. “Reinforced Concrete with FRP Bars: Mechanics and Design,” CRC Press, 2014.

2. Ekenel, M., y Basalo, F. D. C., and Nanni, A. “Fiber-Reinforced Polymer Reinforcement for Concrete Members,” Concrete International, V. 43, No. 2, 2021, pp. 18–22.

3. Salan, A. V., Rahman, M. K., Al-ghamdi, S., et al. “A Monumental Flood Mitigation Channel in Saudi Arabia,” Concrete International, No. October, 2021, pp. 33–41.

4. Classen, M., Hegger, J., Bielak, J., et al. “Shear capacity of continuous concrete slabs with CFRP reinforcement,” V. 320, 2022.

5. Yan, F., Lin, Z., and Yang, M. “Bond mechanism and bond strength of GFRP bars to concrete: A review,” Composites Part B: Engineering, V. 98, 2016, pp. 56–69.

6. Ortiz, J. D., Khedmatgozar Dolati, S. S., Malla, P., et al. “FRP-Reinforced/Strengthened Concrete: State-ofthe-Art Review on Durability and Mechanical Effects,” Materials, V. 16, No. 5, 2023.

7. ACI Committee 440. “Code Requirements for Structural Concrete Reinforced with Glass FRP Bars (ACI 440.11-22),” American Concrete Institute, Farmington Hills, MI., 2022.

8. ASTM Committee D30. “D8505-23, Standard Specification for Basalt and Glass Fiber Reinforced Polymer (FRP) Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA. USA, 2023.

9. Hussain, Z., and Nanni, A. “Design and Detailing of Glass Fiber-Reinforced Polymer-Reinforced Concrete Beams according to ACI 440.11-22,” ACI Structural Journal, 2023.

10. Wambeke, B. W., and Shield, C. K. “Development length of glass fiber-reinforced polymer bars in concrete,” ACI Structural Journal, V. 103, No. 1, 2006, pp. 11–7.

11. ACI Committee 318. “Building Code Requirements for Structural Concrete and Commentary (ACI 318-19),” American Concrete Institute, Farmington Hills, MI., 2019.

12. Orangun, C. O., Jirsa, J. O., and Breen, J. E. “A Reevaluation of Test Data on Development Length and Splices,” ACI Journal Proceedings, V. 74, No. 3, 1977, pp. 114–22.

13. Ruiz Emparanza, A., De Caso, F., and Nanni, A. “Development Length of GFRP Rebars in Reinforced Concrete Members under Flexure,” ACI Symposium Publication, V. 356, 2022.

14. Basaran, B., Kalkan, I., Bergil, E., et al. “Estimation of the FRP-concrete bond strength with code formulations and machine learning algorithms,” Composite Structures, V. 268, No. February, 2021, p. 113972.

15. Pay, A. C., Canbay, E., and Frosch, R. J. “Bond strength of spliced fiber-reinforced polymer reinforcement,” ACI Structural Journal, V. 111, No. 2, 2014, pp. 257–66.

16. Solyom, S., and Balázs, G. L. “Bond of FRP bars with different surface characteristics,” Construction and Building Materials, V. 264, 2020, p. 119839.

17. Rolland, A., Quiertant, M., Khadour, A., et al. “Experimental investigations on the bond behavior between concrete and FRP reinforcing bars,” Construction and Building Materials, V. 173, 2018, pp. 136–48.

18. ACI Committe 440. “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI., 2015.

19. Newman, N., Ayoub, A., and Belarbi, A. “Development length of straight FRP composite bars embedded in concrete,” Journal of Reinforced Plastics and Composites, V. 29, No. 4, 2010, pp. 571–89.

20. Hossain, K. M. A., Ametrano, D., and Lachemi, M. “Bond Strength of Standard and High-Modulus GFRP Bars in High-Strength Concrete,” Journal of Materials in Civil Engineering, V. 26, No. 3, 2014, pp. 449–56.

21. Ametrano, D. “Bond characteristics of glass fibre reinforced polymer bars embedded in high performance and ultra-high performance concrete.” Ryerson University, Toronto, 2011.

22. Abbas, H., Elsanadedy, H., Alaoud, L., et al. “Effect of confining stirrups and bar gap in improving bond behavior of glass fiber reinforced polymer (GFRP) bar lap splices in RC beams,” Construction and Building Materials, V. 365, 2023.

23. Wu, C., Hwang, H. J., and Ma, G. “Effect of stirrups on the bond behavior of lap spliced GFRP bars in concrete beams,” Engineering Structures, V. 266, 2022.

24. ASTM Committee C09. “C39/C39M-21, Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA. USA, 2021.