Specifying Sustainability in Codes for Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Specifying Sustainability in Codes for Concrete Structures

Author(s): Yokota

Publication: Web Session

Volume: ws_S23_Yokota.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/2/2023

Abstract:
Sustainability is a key term to be specified in codes for concrete structures. ISO 22040: 2021 titled “Life cycle management of concrete structures” introduces sustainability indicators for the evaluation of life cycle scenarios at planning, design, execution, use and life-end stages of concrete structures. ISO 19338 titled “Performance and assessment requirements for design standards on structural concrete” is under the process of revision, during which principles of design and assessment with respect to sustainable development and sustainability evaluation are animatedly discussed. Furthermore, in Japan, “Code for the Bases of Structures Design (tentative title)” recommends that the performance requirements of structures should be determined in consideration of social, economic and environmental sustainability. In this presentation these documents will be introduced particularly focusing on how sustainability is dealt with.




  

Edit Module Settings to define Page Content Reviewer