Abstract:
DSC is a valuable tool to study the phase transition temperature and enthalpy of phase change of PCMs that are used in cementitious systems. DSC can be used to characterize PCMs as well as to examine the stability of the enthalpy of phase change. Such data can be used in the modeling of the thermal efficiency of cementitious materials containing phase change materials, as will be explained in this talk.