Synthesis and Analysis of an Anti-Segregation Admixture Based on Acrylamide Copolymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Synthesis and Analysis of an Anti-Segregation Admixture Based on Acrylamide Copolymer

Author(s): Tao Ni, Serina Ng, Zhaoyang Liu, Yongmei Wang, Xin Song, Ke Feng

Publication: Symposium Paper

Volume: 354

Issue:

Appears on pages(s): 347-356

Keywords: acrylamide copolymer; anti-segregation admixture; compressive strength

DOI: 10.14359/51736087

Date: 7/1/2022

Abstract:
Anti-segregation can be employed to avoid the segregation of concrete. Here, we present a type of polymer-based anti-segregation agent, which is the copolymer of acrylamide and 2-acrylamide-2-methylpropane sulfonic acid. The composition and structure were characterized by FT-IR, NMR, and light scattering. Compared with the cellulose derivative, the copolymer can improve not only the homogeneity and bleeding resistance, but also increase the compressive strengths of the concrete by 4 to 5 MPa across all testing periods, up to 28 days. A highlight of the admixture is that can also be used to restore the workability of concrete isolated on site. Finally, the anti-segregation mechanism of the copolymer was analyzed in this article.

Related References:

1. Prakash, N. and Santhanam, M., “A Study of the Interaction between Viscosity Modifying Agent and High Range Water Reducer in Self Compacting Concrete”, Measuring, Monitoring and Modeling Concrete Properties, Netherlands, 2006, pp. 449–454.

2. Piekarczyk, B., “The Type of Air-entraining and Viscosity Modifying Admixtures and Porosity and Frost Durability of High Performance Self-compacting Concrete”, Construction and Building Materials, V.40,2013, pp. 659–671.

3. Shadkam.H.L. and Dadsetan, S., “An Investigation of the Effects of Limestone Powder and Viscosity Modifying Agent in Durability Related Parameters of Self-consolidating Concrete (SCC)”, Construction and Building Materials, V.156, 2017, pp. 152–160.

4. Sonebi, M. and Perrot, A., “Effect of Mix Proportions on Rheology and Permeability of Cement Grouts Containing Viscosity Modifying Admixture”, Construction and Building Materials, V.212, 2019, pp. 687–697.

5. Şahmaran M. and Özkan, N. “Evaluation of Natural Zeolite as a Viscosity-modifying Agent for Cement-based Grouts”, Cement and Concrete Research, V. 38, 2008, pp. 930–937.

6. Benaicha, M. and Roguiez, X., “Influence of Silica Fume and Viscosity Modifying Agent on the Mechanical and Rheological Behavior of Self-compacting Concrete”, Construction and Building Materials, V. 84, 2015, pp. 103–110.

7. Kamal, H. K., “Viscosity-Enhancing Admixtures for Cement-Based Materials - An Overview”, Cement and Concrete Composites, V. 20, 1998, pp. 171-188.

8. Pei, R. and Liu, J., “Use of Bacterial Cell Walls as a Viscosity-modifying Admixture of Concrete”, Cement & Concrete Composites, V. 55, 2015, pp. 186–195.

9. Memon, S.A., Shaikh, M. A., “Utilization of Rice Husk Ash as Viscosity Modifying Agent in Self Compacting Concrete”, Construction and Building Materials, V. 25, 2011, pp. 1044–1048.

10. Leemann, A. and Winnefeld F., “The Effect of Viscosity Modifying Agents on Mortar and Concrete”, Cement & Concrete Composites, V. 29, 2007, pp. 341–34.

11. Lin, S.T. and Huang, R., “Effect of Viscosity Modifying Agent on Plastic Shrinkage Cracking of Cementitious Composites”, Materials and Structures, 2010, V. 43, pp. 651–664.

12. Brumaud, C. and Baumann, R., “Cellulose Ethers and Yield Stress of Cement Pastes”, Cement and Concrete Research, V. 55, 2014, pp. 14–21

13. Sonebi, M., “Rheological Properties of Grouts with Viscosity Modifying Agents as Diutan Gum and Welan Gum Incorporating Pulverised Fly Ash”, Cement and Concrete Research, V. 36, 2006, pp. 1609–1618.

14. Lachemi, M. and Hossain, K.M.A., “Self-consolidating Concrete Incorporating New Viscosity Modifying Admixtures”, Cement and Concrete Research, V. 34, 2004, pp. 917 – 926.

15. Cappellari, M. and Daubreese, A., “Influence of Organic Thickening Admixtures on the Rheological Properties of Mortars: Relationship with Water-retention”, Construction and Building Materials, V. 38, 2013, pp. 950–961.

16. Mohammed, A. and Al-Saadi, N.T.K., “Ultra-High Early Strength Cementitious Grout Suitable for Additive Manufacturing Applications Fabricated by Using Graphene Oxide and Viscosity Modifying Agents”, Polymers, V. 12, 2020, pp. 2900.

17. Khayat, K. H. and Yahiat A., “Effect of Welan gum-high-range Water Reducer Combinations on Rheology of Cement Grout”, ACI Materials Journal, September-October, 1997, pp. 365-37

18. Zhang, J., Gao, X., “Improvement of Viscosity-modifying Agents on Air-void System of Vibrated Concrete”, Construction and Building Materials, V. 239, 2020, pp. 117843.

19. Lothenbach, B. and Winnefeld, F., “Effect of Temperature on the Pore Solution, Microstructure and Hydration Products of Portland Cement Paste”, Cement and Concrete Research. V. 37, 2007, pp. 483–491.

20. Zhang, Y.B., Wu, C. and Fang, Q. et al. “A Light-scattering Study of Aggregation Behavior of Fluorocarbonmodified

Polyacrylamides in Water”. Macromolecules, V. 29, 1996, pp. 2494-2497.