Effect of Different Retarders and their Combination with Superplasticizer on the Properties of CSA

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Different Retarders and their Combination with Superplasticizer on the Properties of CSA

Author(s): A. Govin, G. Quintero, R. Belhadi, P. Grosseau

Publication: Symposium Paper

Volume: 354

Issue:

Appears on pages(s): 143-156

Keywords: CSA, hydration, rheology, admixtures

DOI: 10.14359/51736068

Date: 7/1/2022

Abstract:
The aim of this work was to investigate the effect of polycarboxylate type superplasticizers (PCE), and three different retarders (citric acid, tartaric acid, potassium gluconate) and their combination on the hydration process and rheological properties of CSA at early age. The hydration process was described through isothermal calorimetry, while the rheological properties were characterized through yield stress of cement pastes determined by rheometry. The results show that gluconate is the most powerful retarder, followed by tartaric acid, then citric acid. PCE strongly improves the fluidity of the pastes but a rapid loss of workability is noticed. On the contrary, retarders slightly decrease the yield stress of the pastes but slow down the loss of fluidity. The combination of both admixtures allows for maintaining high fluidity for a longer time. However, for citric acid, and even more for tartaric acid, a rheological instability, characterized by a decrease followed by an increase in the yield stress over time, is noticed. Potassium gluconate seems to be the best retarder to combine with PCE since no instability and longer maintenance of workability were observed. An optimum dosage, leading to the best initial fluidity to the pastes, was also determined for the three retarders. The rheological results are related to the delay induced by the retarder on the hydration product formation for the first hours of hydration and to competitive adsorption between retarder and PCE.

Related References:

1. Damtoft J.S., Lukasik J., Herfort D., Sorrentino D., Gartner E.M., “Sustainable development and climate change initiatives”, Cement and Concrete Research, V. 38, 2008, pp. 115–127.

2. Gartner E., “Industrially interesting approaches to “low-CO2” cements”, Cement and Concrete Research, V. 34, 2004, pp. 1489–1498.

3. Glasser F.P., Zhang L., “High-performance cement matrices based on calcium sulfoaluminate-belite compositions”, Cement and Concrete Research, V. 31, 2001, pp. 1881–1886.

4. Juenger M.C.G., Winnefeld F., Provis J.L., Ideker J.H., “Advances in alternative cementitious binders”, Cement and Concrete Research, V. 41, 2011, pp. 1232–1243.

5. Winnefeld F., Barlag S., “Calorimetric and thermogravimetric study on the influence of calcium sulfate on the hydration of ye’elimite”, Journal of Thermal Analysis and Calorimetry, V. 101, 2010, pp. 949–957.

6. Tan H., Guo Y., Zou F., Jian S., Ma B., Zhi Z., “Effect of borax on rheology of calcium sulphoaluminate cement paste in the presence of polycarboxylate superplasticizer”, Construction and Building Materials, V. 139, 2017, pp. 277–285.

7. Flatt R., “Dispersion forces in cement suspensions”, Cement and Concrete Research, V. 34, 2004, pp. 399–408. Plank J., Winter C., “Competitive adsorption between superplasticizer and retarder molecules on mineral binder surface”, Cement and Concrete Research, V. 38, 2008, pp. 599–605.

8. Plank J., Winter C., “Competitive adsorption between superplasticizer and retarder molecules on mineral binder surface”, Cement and Concrete Research, V. 38, 2008, pp. 599–605.

9. Belhadi R., Govin A., Grosseau P., “Influence of polycarboxylate superplasticizer, citric acid and their combination on the hydration and workability of calcium sulfoaluminate cement”, Cement and Concrete Research, V. 147, No. 106513, 2021.

10. Belhadi R., Grosseau P., Govin A., “Hydration and rheology of sulfoaluminate cements (CSA) in presence of polycarboxylate superplasticizers (PCE) and citric acid”, 15th International Congress on the Chemistry of Cement, 2019.

11. Kutus B., Gaona X., Pallagi A., Pálinkó I., Altmaier M., Sipos P., “Recent advances in the aqueous chemistry of the calcium(II)-gluconate system – Equilibria, structure and composition of the complexes forming in neutral and in alkaline solutions”, Coordination Chemistry Reviews, V. 417, No. 213337, 2020.

12. Gay C., Raphaël E., “Comb-like polymers inside nanoscale pores”, Advances in Colloid and Interface Science, V. 94, 2001, pp. 229–236.

13. Standard EN 196-1, “Methods of testing cement - Part 1: Determination of strength”, 2006.

14. Winnefeld F., “Interaction of superplasticizers with calcium sulfoaluminate cements”, 10th International Conference on Superlasticizers and Other Chemical Admixtures, Volume Supplementary Papers, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, Mich., 2012, pp. 21–36.

15. Ait-Kadi A., Marchal P., Choplin L., Chrissemant A.-S., Bousmina M., “Quantitative analysis of mixer-type rheometers using the Couette analogy”, Canadian Journal of Chemical Engineering, V. 80, 2002, pp. 1166–1174.

16. Phan T.H., Chaouche M., Moranville M., “Influence of organic admixtures on the rheological behaviour of cement pastes”, Cement and Concrete Research, V. 36, 2006, pp. 1807–1813.

17. Roussel N., Ovarlez G., Garrault S., Brumaud C., “The origins of thixotropy of fresh cement pastes”, Cement and Concrete Research, V. 42, 2012, pp. 148–157.

18. Tang S.W., Zhu H.G., Li Z.J., Chen E., Shao H.Y., “Hydration stage identification and phase transformation of calcium sulfoaluminate cement at early age”, Construction and Building Materials, V. 75, 2015, pp. 11–18.

19. Gwon S., Jang S.Y., Shin M., “Combined effects of set retarders and polymer powder on the properties of calcium sulfoaluminate blended cement systems”, Materials, V. 11, No. 825, 2018.

20. Hu Y., Li W., Ma S., Shen X., “Influence of borax and citric acid on the hydration of calcium sulfoaluminate cement”, Chemical Papers, V. 71, 2017, pp. 1909–1919.

21. Telesca A., Marroccoli M., Coppola L., Coffetti D., Candamano S., “Tartaric acid effects on hydration development and physico-mechanical properties of blended calcium sulphoaluminate cements”, Cement and Concrete Composites, V. 124, No. 104275, 2021.

22. Zajac M., Skocek J., Bullerjahn F., Ben Haha M., “Effect of retarders on the early hydration of calcium-sulphoaluminate

(CSA) type cements”, Cement and Concrete Research, V. 84, 2016, pp. 62–75.

23. Zou D., Zhang Z., Wang D., “Influence of citric acid and sodium gluconate on hydration of calcium sulfoaluminate cement at various temperatures”, Construction and Building Materials, V. 263, No. 120247, 2020.