Title:
Study of the Effect of Different Type of Clays on the Initial Flowability of Mortars in the Presence of Polycarboxylate Superplasticizers
Author(s):
Paolo Fornoni, Matteo Destefani, Emanuele Moretti, Francesco Surico, Gilberto Artioli, Maria Chiara Dalconi
Publication:
Symposium Paper
Volume:
355
Issue:
Appears on pages(s):
271-282
Keywords:
Clay bearing sand, polycarboxylate superplasticizers, sustainability, Methylene Blue test
DOI:
10.14359/51736033
Date:
7/1/2022
Abstract:
The presence of impurities, particularly clays, in sands and aggregates can severely affect the performances of the superplasticizers, particularly polycarboxylate (PCEs). Due to both the large specific surface and the possibility to intercalate the polyoxyethylene side chains of PCEs, clays can capture a large amount of PCEs and correspondingly decrease their efficiency in dispersing the cement particles. From the analytical point of view, the Methylene Blue value (MBV) is the most well-recognized field test to quantify the clay content in the sands. In this work, the MBV of several clays and sands collected from job sites (technical sands) with different origins and lithology was measured and the loss of the initial flowability of mortars prepared with these sands and clays was evaluated. Results indicated that the loss of initial flowability of the mortars, in which the standard sand was partially replaced only by clays, was directly related to the MBV. For the mortars prepared with the technical sands, this direct relationship was not verified: other parameters like the mineralogical composition of the sands tested, their particle size distribution, surface water absorption, and ultra-fine content < 0.075 mm (0.03 in.) could contribute to determining their flow behavior.
Related References:
1. S. Ng and J. Plank, "Interaction mechanisms between Na montmorillonite clay and MPEG-based polycarboxylate superplasticizers" Cement and Concrete Research, vol. 42, pp. 847-854, 2012.
2. Nedhi, M. L. “Clay in cement-based material: critical overview of the state of the art” Construction and building material, 51, pp. 372-382, 2014
3. Chiappone A., Scavia Claudio. “La prova al blu di metilene nella caratterizzazione geotecnica: un'applicazione allo studio della stabilità dei versanti” Rivista italiana di geotecnica 4/99, 37-51, 1999.
4. Klein, C., Manual of Mineral Science, 2014, Zanichelli.
5. Schwartzentruber A., Chaterine C. “La méthode du mortier de béton équivalent (MBE) – Un nouvel outil d’aide à la formulation des béton adjuvantés” Materials and Structures, vol 23, October, pp 475-482, 2000.
6. Döbelin, N. K. “Profex: a graphical user interface for the Rietveld refinement program BGMN” Journal of Applied Crystallography 48, 1573-1580, 2015.
7. Justin K. Norvell, J. G. (s.d.). “Influence of clays and clay-sized particles on concrete performance” Journal of materials in civil engeneering, 19, pp. 1053-1059, December 2007.
8. Vasavithansan M., W. D. “Qualitative assessment of aggregate for presence of clay” Materials engineering and research office, 51, 2005.
9. Fairbairn PE, R. R. “Liquid limit and dyes adsorption”. Clay mineral bull, 129-36, 1957.
10. PNW, V. “The methylene blue adsorption test applied to geo-materials” Technische Universiteit Delft. Report No. MAO-R-92025.1992D.,
11. Lautrin. “Une Procédure rapide d'identification des argiles” Bulletin de laison des Laboratoires des ponts et chaussées” n 152, novembre-décembre, 75-84, 1987
12. EN 933-1:2012 Tests for geometrical properties of aggregates - Part 1: Determination of particle size distribution - Sieving method
13. EN 197-1:2011 Cement - Part 1: Composition, specifications and conformity criteria for common cements
14. EN 196-1:2016 Methods of testing cement - Part 1: Determination of strength
15. ASTM C1777-15 Standard Test Method For Rapid Determination Of The Methylene Blue Value For Fine Aggregate Or Mineral Filler Using A Colorimeter
16. EN 1097-6:2013 Tests for mechanical and physical properties of aggregates - Part 6: Determination of particle density and water absorption Methods of testing cement - Part 1: Determination of strength