Seismic Performance of Precast Multi-span Frame System Integrated by Unbonded Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance of Precast Multi-span Frame System Integrated by Unbonded Tendons

Author(s): Jae Hyun Kim, Deuckhang Lee, Seung-Ho Choi, Hoseong Jeong, and Kang Su Kim

Publication: Structural Journal

Volume: 119

Issue: 5

Appears on pages(s): 193-206

Keywords:

DOI: 10.14359/51734801

Date: 9/1/2022

Abstract:
In this study, three multi-span moment frames are fabricated and tested under reversed cyclic loadings. The test program includes a reinforced concrete (RC) specimen with typical monolithic connections, which fully satisfies the seismic specification of the special moment frame prescribed in ACI 318, and two hybrid posttensioned precast concrete (HPPC) frame specimens, which are integrated using unbonded prestressing tendons throughout two-bay continuous spans. On this basis, excellent structural integrity and connection continuities in beam-column joints between discrete precast members can be achieved. The HPPC frame systems demonstrate seismic performances that are comparable to those of monolithic RC special moment frames designed based on the seismic design provision specified in ACI 318. In addition, key observations from the test program are presented comprehensively, where quantitative indexes are used to evaluate the seismic performance of the test specimens in terms of capacity, ductility, and damage characteristics, and the cyclic responses of the HPPC specimens were verified by using numerical analyses.

Related References:

1. Priestley, M. J. N., “Overview of PRESSS Research Program,” PCI Journal, V. 36, No. 4, 1991, pp. 50-57. doi: 10.15554/pcij.07011991.50.57

2. Priestley, M. J. N., and Tao, J. R., “Seismic Response of Precast Prestressed Concrete Frames with Partially Debonded Tendons,” PCI Journal, V. 38, No. 1, 1993, pp. 58-69. doi: 10.15554/pcij.01011993.58.69

3. Palmieri, L.; Saqan, E.; French, C.; and Kreger, M., “Ductile Connections for Precast Concrete Frame Systems,” Mete A. Sozen Symposium: A Tribute from His Students, SP-162, J. K. Wight and M. Kreger, eds., American Concrete Institute, Farmington Hills, MI, 1996, pp. 313-356.

4. Nakaki, S. D.; Stanton, J. F.; and Sritharan, S. S., “An Overview of the PRESSS Five-Story Precast Test Building,” PCI Journal, V. 44, No. 2, 1999, pp. 26-39. doi: 10.15554/pcij.03011999.26.39

5. El-Sheikh, M. T.; Sause, R.; Pessiki, S.; and Lu, L.-W., “Seismic Behavior and Design of Unbonded Post-Tensioned Precast Concrete Frames,” PCI Journal, V. 44, No. 3, 1999, pp. 54-71. doi: 10.15554/pcij.05011999.54.71

6. Priestley, M. J. N.; Sritharan, S. S.; Conley, J. R.; and Pampanin, S., “Preliminary Results and Conclusions from the PRESSS Five-Story Precast Concrete Test Building,” PCI Journal, V. 44, No. 6, 1999, pp. 42-67. doi: 10.15554/pcij.11011999.42.67

7. Nakano, K.; Tanabe, K.; Matsuzaki, Y.; Wada, A.; Sakata, H.; and Kuboyama, H., “Experimental Study on Mechanical Behavior of Damage Controlled Precast-Prestressed Concrete Structure with P/C MILD PRESS-JOINT,” Proceedings of the 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada, Paper No. 2778, 2004, 12 pp.

8. Qian, K.; Liang, S.-L.; Feng, D.-C.; Fu, F.; and Wu, G., “Experimental and Numerical Investigation on Progressive Collapse Resistance of Post-Tensioned Precast Concrete Beam-Column Subassemblages,” Journal of Structural Engineering, ASCE, V. 146, No. 9, 2020, pp. 1-19. doi: 10.1061/(ASCE)ST.1943-541X.0002714

9. Wang, H.; Marino, E. M.; Pan, P.; Liu, H.; and Nie, X., “Experimental Study of a Novel Precast Prestressed Reinforced Concrete Beam-to-Column Joint,” Engineering Structures, V. 156, 2018, pp. 68-81. doi: 10.1016/j.engstruct.2017.11.011

10. Morgen, B. G., and Kurama, Y. C., “A Friction Damper for Post-Tensioned Precast Concrete Beam-to-Column Joints,” Proceedings of the 13th World Conference on Earthquake Engineering, Vancouver, BC, Canada, Paper No. 3189, 2004, 15 pp.

11. Kaya, M., and Arslan, A. S., “Analytical Modeling of Post-Tensioned Precast Beam-to-Column Connections,” Materials & Design, V. 30, No. 9, 2009, pp. 3802-3811. doi: 10.1016/j.matdes.2009.01.033

12. Song, B.; Xu, W.; Du, D.; Wang, S.; Li, W.; and Zhang, Y., “Seismic Design of Hybrid Unbonded Post-Tensioned Precast Concrete Joints Based on Bearing Capacity and Energy Dissipation Capacity,” Advances in Structural Engineering, V. 24, No. 8, 2021, pp. 1724-1738. doi: 10.1177/1369433220982733

13. Kurosawa, R.; Sakata, H.; Qu, Z.; and Suyama, T., “Precast Prestressed Concrete Frames for Seismically Retrofitting Existing RC Frames,” Engineering Structures, V. 184, 2019, pp. 345-354. doi: 10.1016/j.engstruct.2019.01.110

14. Kim, J. H.; Choi, S.-H.; Hwang, J.-H.; Jeong, H.; Han, S.-J.; and Kim, K. S., “Experimental Study on Lateral Behavior of Post-Tensioned Precast Beam-Column Joints,” Structures, V. 33, 2021, pp. 841-854. doi: 10.1016/j.istruc.2021.04.095

15. Choi, S.-H.; Hwang, J.-H.; Heo, I.; Kim, K. S.; and Woo, W.-T., “Flexural Response of Negative Moment Region of Hybrid Prestressed Precast Concrete (HPPC) System,” Journal of the Architectural Institute of Korea Structure & Construction, V. 34, No. 10, 2018, pp. 3-10. doi: 10.5659/JAIK_SC.2018.34.10.3

16. Kaya, M., and Arslan, A. S., “The Effect of the Diameter of Prestressed Strands Providing the Post-Tensioned Beam-to-Column Connections,” Materials & Design, V. 30, No. 7, 2009, pp. 2604-2617. doi: 10.1016/j.matdes.2008.11.012

17. Jin, K.; Kitayama, K.; Song, S.; and Kanemoto, K., “Shear Capacity of Precast Prestressed Concrete Beam-Column Joint Assembled by Unbonded Tendon,” ACI Structural Journal, V. 114, No. 1, Jan.-Feb. 2017, pp. 51-62. doi: 10.14359/51689148

18. Song, M.; He, J.; Liu, Y.; Zhang, H.; Ge, C.; Jin, Y.; Liu, B.; Huang, S.; and Liu, Y., “Seismic Behavior of Three-Story Prestressed Fabricated Concrete Frame under Dynamic and Low Reversed Cyclic Loading,” Advances in Civil Engineering, V. 2018, 2018, 10 pp. doi: 10.1155/2018/7876908

19. Rha, C.; Kang, T. H.-K.; Shin, M.; and Yoon, J. B., “Gravity and Lateral Load-Carrying Capacities of Reinforced Concrete Flat Plate Systems,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 753-764. doi: 10.14359/51686731

20. Park, R., and Thompson, K. J., “Cyclic Load Tests on Prestressed and Partially Prestressed Beam-Column Joints,” PCI Journal, V. 22, No. 5, 1977, pp. 84-110. doi: 10.15554/pcij.09011977.84.110

21. Harajli, M. H., “Behavior of Partially Prestressed Concrete Joints under Cyclic Loading,” Journal of Structural Engineering, ASCE, V. 114, No. 11, 1988, pp. 2525-2543. doi: 10.1061/(ASCE)0733-9445(1988)114:11(2525)

22. Astawa, M. D.; Tavio.; and Raka, I. G. P., “Ductile Structure Framework of Earthquake Resistant of Highrise Building on Exterior Beam-Column Joint with the Partial Prestressed Concrete Beam-Column Reinforced Concrete,” The 2nd International Conference on Rehabilitation and Maintenance in Civil Engineering, V. 54, F. Nestmann, E. Schlangen, and S. As’ad, eds., 2013, pp. 413-427. doi: 10.1016/j.proeng.2013.03.037

23. Zerbe, H. E., and Durrani, A. J., “Seismic Response of Connections in Two-Bay R/C Frame Subassemblies,” Journal of Structural Engineering, ASCE, V. 115, No. 11, 1989, pp. 2829-2844. doi: 10.1061/(ASCE)0733-9445(1989)115:11(2829)

24. Zerbe, H. E., and Durrani, A. J., “Seismic Response of Connections in Two-Bay Reinforced Concrete Frame Subassemblies with a Floor Slab,” ACI Structural Journal, V. 87, No. 4, July-Aug. 1990, pp. 406-415. doi: 10.14359/3046

25. Kabeyasawa, T.; Sanada, Y.; and Maeda, M., “Effect of Beam Axial Deformation on Column Shear in Reinforced Concrete Frames,” Proceedings of the 12th World Conference on Earthquake Engineering, Auckland, New Zealand, Paper No. 1017, 2000, 8 pp.

26. Kim, J.; Stanton, J.; and MacRae, G., “Effect of Beam Growth on Reinforced Concrete Frames,” Journal of Structural Engineering, ASCE, V. 130, No. 9, 2004, pp. 1333-1342. doi: 10.1061/(ASCE)0733-9445(2004)130:9(1333)

27. Wang, L.; Tian, Y.; Luo, W.; Li, G.; Zhang, W.; Liu, S.; and Zhang, C., “Seismic Performance of Axially Restrained Reinforced Concrete Frame Beams,” Journal of Structural Engineering, ASCE, V. 145, No. 5, 2019, pp. 1-12. doi: 10.1061/(ASCE)ST.1943-541X.0002306

28. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

29. ACI Committee 374, “Acceptance Criteria for Moment Frames Based on Structural Testing and Commentary (ACI 374.1-05) (Reapproved 2019),” American Concrete Institute, Farmington Hills, MI, 2005, 9 pp.

30. Ozden, S.; Akguzel, U.; and Ozturan, T., “Seismic Strengthening of Infilled Reinforced Concrete Frames with Composite Materials,” ACI Structural Journal, V. 108, No. 4, July-Aug. 2011, pp. 414-422. doi: 10.14359/51682981

31. Choi, S.-H.; Hwang, J.-H.; Lee, D. H.; Kim, K. S.; Zhang, D.; and Kim, J. R., “Experimental Study on RC Frame Structures Strengthened by Externally-Anchored PC Wall Panels,” Computers and Concrete, V. 22, No. 4, 2018, pp. 383-393. doi: 10.12989/cac.2018.22.4.383

32. Feng, F.; Jiang, K.; Hwang, H.-J.; and Yi, W.-J., “Earthquake Response of Low-Rise RC Moment Frame Structures according to Energy Dissipation Ratio of Beam-Column Joints,” Journal of Structural Integrity and Maintenance, V. 3, No. 1, 2018, pp. 33-43. doi: 10.1080/24705314.2018.1426171

33. Hwang, T.-H., “Effects of Variation in Load History on Cyclic Response of Concrete Flexural Members,” PhD thesis, University of Illinois at Urbana-Champaign, Urbana, IL, 1982, 231 pp.

34. Jacobsen, L. S., “Steady Forced Vibrations as Influenced by Damping,” ASME Transactions, V. 52, No. 1, 1930, pp. 169-181.

35. Oudah, F., and El-Hacha, R., “Damage and Deformation Assessment of Earthquake-Resistant RC Slotted Beam-Column Connections Using Digital Image Correlation Technique,” Engineering Structures, V. 215, 2020, Article No. 110442, 14 pp. doi: 10.1016/j.engstruct.2020.110442

36. Priestley, M. J. N., and Grant, D. N., “Viscous Damping in Seismic Design and Analysis,” Journal of Earthquake Engineering, V. 9, No. sup2, 2005, pp. 229-255. doi: 10.1142/S1363246905002365

37. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

38. Cao, V. V.; Ronagh, H. R.; Ashraf, M.; and Baji, H., “A New Damage Index for Reinforced Concrete Structures,” Earthquakes and Structures, V. 6, No. 6, 2014, pp. 581-609. doi: 10.12989/eas.2014.6.6.581

39. Roufaiel, M. S. L., and Meyer, C., “Analysis of Damaged Concrete Frame Buildings,” Technical Report No. NSF-CEE-81-21359-1, Columbia University, New York, NY, 1983, 164 pp.

40. Kim, T.-H.; Lee, K.-M.; Chung, Y.-S.; and Shin, H. M., “Seismic Damage Assessment of Reinforced Concrete Bridge Columns,” Engineering Structures, V. 27, No. 4, 2005, pp. 576-592. doi: 10.1016/j.engstruct.2004.11.016

41. Mergos, P. E., and Kappos, A. J., “Seismic Damage Analysis Including Inelastic Shear-Flexure Interaction,” Bulletin of Earthquake Engineering, V. 8, No. 1, 2010, Article No. 27. doi: 10.1007/s10518-009-9161-2

42. Park, Y.-J., and Ang, A. H.-S., “Mechanistic Seismic Damage Model for Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 111, No. 4, 1985, pp. 722-739. doi: 10.1061/(ASCE)0733-9445(1985)111:4(722)

43. Hait, P.; Sil, A.; and Choudhury, S., “Seismic Damage Assessment and Prediction Using Artifical Neural Network of RC Building Considering Irregularities,” Journal of Structural Integrity and Maintenance, V. 5, No. 1, 2020, pp. 51-69. doi: 10.1080/24705314.2019.1692167

44. FEMA 356, “Prestandard and Commentary for the Seismic Rehabilitation of Buildings,” Federal Emergency Management Agency, Washington, DC, 2000, 518 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal