Title: Confining Concrete Column with Eco-friendly UHPC

Author(s): Fantilli

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/1/2021

Abstract:
UHPC shows excellent mechanical performances and has been successfully used for repairing, strengthening, and seismic retrofitting of old structures. However, UHPC is not always an environmentally friendly product, due to the large quantity of cement contained in the mixture. Thus, different rates of fly ash substitute herein part of the cement, and new UHPCs are used to retrofit concrete columns. Specifically, to simulate the mechanical response of confined columns, cylindrical specimens, made of normal concrete and reinforced with different UHPC jackets, are tested in uniaxial compression. Relationships between the size of the jacket, the percentage of cement replaced by fly ash, and the strength of the columns are measured and analyzed by means of the eco-mechanical approach. As a result, a replacement of approximately 50% of cement with fly ash, and a suitable thickness of the UHPC jacket, might ensure the lowest environmental impact without compromising the mechanical performances.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer