Abstract:
A layer of 2-4 mm (0.08-0.16 in) protective render coat (PRC) has proven to be an effective anticarbonation barrier at two bridges protecting the underlying concrete against carbonation for 100 years. The carbonation of concrete under the PRC with low permeability was found to be less than 2 mm (0.08 in). It is assumed that the PRC was placed for aesthetic purposes. Taking into account the considered XC3 exposure class
according to EN 206, to which concrete structures were subjected and compressive strengths of the underlying concrete between 20 - 25 MPa (2900 - 3625 psi), low carbonation depth can be explained by the presence of the PRC applied on concrete surface. The main scientific goal of this article is to explain the cause of extremely low carbonation depth of concrete under the PRC. Its composition has been unknown until now but the present research reveals the secret of this substance. Investigations of the aspects of low carbonation depth thoroughly focused on the PRC role covering concrete beneath as well as material development of new current PRC based on the present cement and sand, without the use of chemical admixtures, are also the subject of ongoing research.
Related References:
1. fib Bulletin 34, 2006, “Model code for service life design. Fédération internationale du béton (fib)“, Lausanne, Switzerland, 116 p.
2. Shah, V., and Bishnoi, S., 2018, “Carbonation resistance of cements containing supplementary materials and its relation to various parameters of concrete”, Construction and Building Materials, 178(7), 219-232.
3. Suvash, C. P., Biranchi, P., Yuhao H., Akhil, G., and Xiongbin, P., 2018, “An empirical model design for evaluation of carbonation depth in concrete”, Measurement, 124(8), 205-210.
4. Ribeiro A.B., Santos T., and Gonꞔalves A., 2018, “Performance of concrete exposed to natural carbonation: Use of the k-value concept”, Construction and Building Materials, 175(6), 360-370.
5. STN EN 206 + A1, 2017, “Concrete. Specification, performance, production and conformity”, (in Slovak), Slovak Office of Standards, Metrology and Testing in Bratislava.
6. Paulík, P., Bačuvčík, M., Ševčík, P., and Janotka, I., 2016, “Material properties study of seven 100-years old concrete bridges in Slovakia”, Proceedings of fib Symposium 2016 Performance - Based Approaches for Concrete
Structures, Cape Town, South Africa, Chapter 12: Condition Assessment, Article No. 218.
7. Janotka, I., Ševčík, P., Paulík, P., and Bačuvčík, M., 2015, “Verification of concrete durability of 124 year old bridge in Bratislava”, Proceedings of Thirteenth International Conference on Recent Advances in Concrete Technology and Sustainability Issues, Supplementary Papers, Ottawa, Canada, July 14-17, 2015, 173-190.
8. Paulík, P., Bačuvčík, M., Ševčík, P., and Janotka, I., 2016, “Material properties and carbonation depths on seven, more than a 100-years old, concrete bridges in Slovakia”, Procedia Engineering, 156, 326-333.
9. Janotka, I., Bačuvčík, M., Ševčík P., and Paulík, P., 2016, “Physical and chemical state of 124 - years old reinforced concrete bridge”, Proceedings of Ninth International Conference Concrete Days, Vol. 1 Wisla, Poland, October 10-12, 2016, 509-524.
10. STN 73 1373, 1981, “ Testing of concrete by hardness testing methods”, (in Slovak), Slovak Office of Standards, Metrology and Testing in Bratislava.
11. STN 73 1371, 1981, “Method of ultrasonic pulse testing of concrete”, (in Slovak), Slovak Office of Standards, Metrology and Testing in Bratislava.
12. STN EN 12636, 2001, “Products and systems for the protection and repair of concrete structures. Test methods. Determination of adhesion concrete to concrete”, (in Slovak), Slovak Office of Standards, Metrology and Testing in Bratislava.
13. Torrent, R., and Frenzer, G., 1995, “Study on methods to determine and judge characteristic values of the cover concrete on site”, (in German), Bundesamt für Strassenbau, Bern, 516, 105 p.
14. Janotka, I., Bačuvčík, M., and Paulík, P., 2018, “Low carbonation of concrete found on 100-years-old bridges”, Case Studies in Construction Materials, 8, June 2016, 97-115.
15. STN 72 0101, 1973, “Basic analysis of silicates. Common regulations”, Slovak Office of Standards, Metrology and Testing in Bratislava.
16. Matoušek, M., and Drochytka, R., 1998, “Atmospheric corrosion of concrete” (in Czech), IKAS – ČKAIT, Prague, 171 p.
17. Janotka, I., and Krajči, L., 1998, “Concrete deterioration determined by four stages of carbonation”, Proceedings of Thirteenth FIP Congress on Challenges for Concrete in the Next Millennium, Amsterdam, The Netherlands, 1051-1054.
18. Krajči, L., and Janotka, I., 2000, “Measurement techniques for rapid assessment of carbonation in concrete”, ACI Materials. Journal, 97(2), 168-171.
19. STN 73 1323, 1989, “Determination of concrete components”, (in Slovak), Slovak Office of Standards, Metrology and Testing in Bratislava.