Performance of TRM/TRC systems under elevated temperatures and fire conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Performance of TRM/TRC systems under elevated temperatures and fire conditions

Author(s): Catherine (Corina) Papanicolaou and Thanasis Triantafillou

Publication: Symposium Paper

Volume: 345

Issue:

Appears on pages(s): 32-46

Keywords: TRM, TRC, elevated/high temperatures, fire

DOI: 10.14359/51731569

Date: 2/1/2021

Abstract:
In this paper, authors draw information from previous work aiming at contributing to: (i) a summary of the existing knowledge on the mechanical performance of TRM/TRC systems under elevated temperatures and fire conditions; and (ii) highlighting the most important issues of testing procedures and protocols. The paper refers to both TRM- and TRC-related data. The former include experimental assessments of the: (a) TRM-to-substrate residual bond characteristics as a function of temperature; and (b) structural performance of fired masonry elements furnished with a new type of TRM-based overlay for combined structural and energy upgrading. TRC-related data focus on the structural degradation of thin TRC plates under both standard and non-standard fire conditions.

Related References:

1. Pancar, E.B. & Akpınar, M.V. Int J Concr Struct Mater (2016) 10: 39. doi: 10.1007/s40069-016-0130-2

2. Oxfall, M. (2016). Climatic conditions inside nuclear reactor containments: Evaluation of moisture condition in the concrete within reactor containments and interaction with the ambient compartments. Lund.

3. Naus, D.J., 2006. The effect of elevated temperature on concrete materials and structures-a literature review (No. ORNL/TM--2005/553). Oak Ridge National Laboratory (United States). Funding organisation: ORNL work for others (United States).

4. FIB Bulletin 38, 2007. Fire design of concrete structures-materials, structures and modeling. The International Federation for Structural Concrete.

5. Ehlig, D., Jesse, F. and Curbach, M., 2010, September. High temperature tests on textile reinforced concrete (TRC) strain specimens. In International RILEM Conference on Material Science (pp. 141-151). RILEM Publications SARL.

6. Colombo, I., Colombo, M., Magri, A., Zani, G. and di Prisco, M., 2011. Textile reinforced mortar at high temperatures. In Applied mechanics and materials (Vol. 82, pp. 202-207). Trans Tech Publications.

7. de Andrade Silva, F., Butler, M., Hempel, S., Toledo Filho, R.D. and Mechtcherine, V., 2014. Effects of elevated temperatures on the interface properties of carbon textile-reinforced concrete. Cement and Concrete Composites, 48, pp.26-34.

8. Rambo, D.A.S., de Andrade Silva, F., Toledo Filho, R.D. and Gomes, O.D.F.M., 2015. Effect of elevated temperatures on the mechanical behavior of basalt textile reinforced refractory concrete. Materials & Design (1980-2015), 65, pp.24-33.

9. Nguyen, T.H., Vu, X.H., Larbi, A.S. and Ferrier, E., 2016. Experimental study of the effect of simultaneous mechanical and high-temperature loadings on the behaviour of textile-reinforced concrete (TRC). Construction and Building Materials, 125, pp.253.

10. Rambo, D.A.S., de Andrade Silva, F., Toledo Filho, R.D., Ukrainczyk, N. and Koenders, E., 2016. Tensile strength of a calcium-aluminate cementitious composite reinforced with basalt textile in a high-temperature environment. Cement and Concrete Composites, 70, pp.183-193.

11. Rambo, D.A.S., Yao, Y., de Andrade Silva, F., Toledo Filho, R.D. and Mobasher, B., 2017. Experimental investigation and modelling of the temperature effects on the tensile behavior of textile reinforced refractory concretes. Cement and Concrete Composites, 75, pp.51-61.

12. Homoro, O., Vu, X.H. and Ferrier, E., 2018. Experimental and analytical study of the thermo-mechanical behaviour of textile-reinforced concrete (TRC) at elevated temperatures: Role of discontinuous short glass fibres. Construction and Building Materials, 190, pp.645-663.

13. Tlaiji, T., Vu, X.H., Ferrier, E. and Larbi, A.S., 2018. Thermomechanical behaviour and residual properties of textile reinforced concrete (TRC) subjected to elevated and high temperature loading: Experimental and comparative study. Composites Part B: Engineering, 144, pp.99-110.

14. Messori, M., Nobili, A., Signorini, C. and Sola, A., 2019. Effect of high temperature exposure on epoxy-coated glass textile reinforced mortar (GTRM) composites. Construction and Building Materials, 212, pp.765-774.

15. Truong, G.T., Park, S.H. and Choi, K.K., 2019. Tensile Behaviors of Lap-Spliced Carbon Fiber-Textile Reinforced Mortar Composites Exposed to High Temperature. Materials, 12(9), p.1512.

16. Tran, M.T., Vu, X.H. and Ferrier, E., 2019. Mesoscale experimental investigation of thermomechanical behaviour of the carbon textile reinforced refractory concrete under simultaneous mechanical loading and elevated temperature. Construction and Building Materials, 217, pp.156-171.

17. Antons, U., Hegger, J., Kulas, C. and Raupach, M., 2012, June. High-temperature tests on concrete specimens reinforced with alkali-resistant glass rovings under bending loads. In Proceedings of the 6th International Conference on FRP Composites in Civil Engineering, Rome, Italy (pp. 13-15).

18. Xu, S.L., Shen, L.H., Wang, J.Y. and Fu, Y., 2014. High temperature mechanical performance and micro interfacial adhesive failure of textile reinforced concrete thin-plate. Journal of Zhejiang University SCIENCE A, 15(1), pp.31-38.

19. Xu, S., Shen, L. and Wang, J., 2016. The high-temperature resistance performance of TRC thin-plates with different cementitious materials: Experimental study. Construction and Building Materials, 115, pp.506-519.

20. Li, T., Zhang, Y. and Dai, J.G., 2017. Flexural behavior and microstructure of hybrid basalt textile and steel fiber reinforced alkali-activated slag panels exposed to elevated temperatures. Construction and Building Materials, 152, pp.651-660.

21. Kapsalis, P., Tysmans, T., Verbruggen, S. and Triantafillou, T., 2018. Preliminary High-Temperature Tests of Textile Reinforced Concrete (TRC). In Multidisciplinary Digital Publishing Institute Proceedings (Vol. 2, No. 8, p. 522).

22. Kapsalis, P., El Kadi, M., Vervloet, J., De Munck, M., Wastiels, J., Triantafillou, T. and Tysmans, T., 2019. Thermomechanical Behavior of Textile Reinforced Cementitious Composites Subjected to Fire. Applied Sciences, 9(4), p.747.

23. Ombres, L., 2015. Analysis of the bond between fabric reinforced cementitious mortar (FRCM) strengthening systems and concrete. Composites Part B: Engineering, 69, pp.418-426.

24. Maroudas, S.R. and Papanicolaou, C.C.G., 2017. Effect of high temperatures on the TRM-to-masonry bond. In Key Engineering Materials (Vol. 747, pp. 533-541). Trans Tech Publications.

25. Raoof, S.M. and Bournas, D.A., 2017. Bond between TRM versus FRP composites and concrete at high temperatures. Composites Part B: Engineering, 127, pp.150-165.

26. Donnini, J., y Basalo, F.D.C., Corinaldesi, V., Lancioni, G. and Nanni, A., 2017. Fabric-reinforced cementitious matrix behavior at high-temperature: Experimental and numerical results. Composites Part B: Engineering, 108, pp.108-121.

27. Ombres, L., Iorfida, A., Mazzuca, S. and Verre, S., 2018. Bond analysis of thermally conditioned FRCM-masonry joints. Measurement, 125, pp.509-515.

28. Askouni, P.D., Papanicolaou, C.C.G. and Kaffetzakis, M.I., 2019. The Effect of Elevated Temperatures on the TRM-to-Masonry Bond: Comparison of Normal Weight and Lightweight Matrices. Applied Sciences, 9(10), p.2156.

29. Bisby, L., Stratford, T., Smith, J. and Halpin, S., 2010. Comparative performance of fibre reinforced polymer and fibre reinforced cementitious mortar strengthening systems in elevated temperature service environments. Structural Faults and Repair.

30. Bisby, L., Stratford, T., Hart, C. and Farren, S., 2013. Fire performance of well-anchored TRM, FRCM and FRP flexural strengthening systems. Adv Compos Constr.

31.Michels, J., Zwicky, D., Scherer, J., Harmanci, Y.E. and Motavalli, M., 2014. Structural strengthening of concrete with fiber reinforced cementitious matrix (FRCM) at ambient and elevated temperature—Recent investigations in Switzerland. Advances in Structural Engineering, 17(12), pp.1785-1799.

32. Raoof, S.M. and Bournas, D.A., 2017. TRM versus FRP in flexural strengthening of RC beams: Behaviour at high temperatures. Construction and Building Materials, 154, pp.424-437.

33. Triantafillou, T.C., Karlos, K., Kefalou, K. and Argyropoulou, E., 2017. An innovative structural and energy retrofitting system for URM walls using textile reinforced mortars combined with thermal insulation: Mechanical and fire behavior. Construction and Building Materials, 133, pp.1-13.

34. Tetta, Z.C. and Bournas, D.A., 2016. TRM vs FRP jacketing in shear strengthening of concrete members subjected to high temperatures. Composites Part B: Engineering, 106, pp.190-205.

35. Trapko, T., 2013. The effect of high temperature on the performance of CFRP and FRCM confined concrete elements. Composites Part B: Engineering, 54, pp.138-145.

36. Papanicolaou, C., Kaffetzakis, M., Kollia, K. and Polyzou, D. (2016), Deliverable WP10, ‘Prescient’ Project: "Paradigm for Resilient Concrete Infrastructures to Extreme Natural and Man-made Threats", National Strategic Reference Framework (NSRF) 2007-2013 (Project leader: Prof. Fardis).

37. Al-Salloum, Y.A., Almusallam, T.H., Elsanadedy, H.M. and Iqbal, R.A., 2016. Effect of elevated temperature environments on the residual axial capacity of RC columns strengthened with different techniques. Construction and Building Materials, 115, pp.345-361.

38. Ombres, L., 2017. Structural performances of thermally conditioned PBO FRCM confined concrete cylinders. Composite Structures, 176, pp.1096-1106.

39. EN 1363-1, Fire resistance tests – Part 1: general requirements, European Committee for Standardization, Brussels, 1999.