Abstract:
The use of fiber reinforced concrete in tunnel linings, with or without conventional rebars, has increased in the two last decades, especially in segmental linings. In the meanwhile, in the scientific community there was a growing interest on macro-synthetic fibers for use in
underground structures. Within this framework, the present study investigates the possibility of using macro-synthetic fiber reinforcement in precast tunnel segments by means of a
numerical study. Firstly, an experimental program based on three point bending tests was carried out on polypropylene fiber reinforced concretes (PFRCs) characterized by different fiber contents in order to assess their post-cracking residual strength. Secondly, the corresponding stress vs. crack opening laws, representative of the PFRCs investigated, were calculated through
inverse analysis procedure. Then, a segment of a typical tunnel lining having small diameter was adopted as reference to optimize the reinforcement solution (macro-synthetic fibers and conventional rebars, i.e. hybrid solution) and to study its structural behavior by numerical analyses. Particular attention was devoted to the Tunnel Boring Machine (TBM) thrust jack phase, in which the TBM moves forward by pushing the thrust jacks on the bearing pads of
the latest assembled ring, introducing high-concentrated forces in the lining.
Related References:
ACI Committee 544 R16 (2016), Report on Design and Construction of Fiber Reinforced Precast Concrete Tunnel Segments, ACI 544.7R-16, American Concrete Institute, pp. 36.
Blom C.B.M. (2002), Design philosophy of concrete linings for tunnels in soft soils, Ph.D Thesis, Delft University of Technology, The Netherlands, pp. 184.
Conforti, A., Minelli, F., Plizzari, G.A., and Tiberti, G. (2017), Comparing test methods for the mechanical characterization of fiber reinforced concrete, Structural Concrete, 1-14,
doi: 10.1002/suco.201700057
Conforti, A., Tiberti, G., Plizzari, G.A., Caratelli, A., and Meda A. (2017), Precast tunnel segments reinforced by macro-synthetic fibers, Tunnelling and Underground Space Technology, Vol. 63, pp. 1-11.
DIANA – Finite Element Analysis (2016), User’s Manual release 10.1. TNO DIANA BV, Delft, The Netherlands. Edited by Jonna Manie and Wijtze Pieter Kikstra.
EN 14651 (2005), Precast concrete products – test method for metallic fibre concrete – Measuring the flexural tensile strength. European Standard. Eurocode 2 (2004), Design of concrete structures. European Standard.
fib Bulletin 83 (2017), Precast tunnel segments in fibre-reinforced concrete, W.P. 1.4.1 Tunnels in fiber reinforced concrete, ISSN 1562-3610, ISBN 978-2-88394-123-6.
Groeneweg T.W. (2007), Shield driven tunnels in ultra high strength concrete, reduction of the tunnel lining thickness, Graduate Thesis, Delft University of Technology, The Netherlands, January, 2007.
ITA report n. 16 (2016), Twenty years of FRC tunnel segments practice: lessons learnt and proposed design principles, April 2016, pp. 71, ISBN 978-2-970-1013-5-2.
Liao L., De la Fuente A., Cavalaro S. and Aguado, A. (2015), Design of FRC tunnel segments considering the ductility requirements of the Model Code 2010, Tunnelling and Underground Space Technology, Vol. 47, pp. 200-210.
Model Code 2010 - Final draft (2012), fib Bulletin 65. Volume 1, pp. 350, ISBN 978-2-88394-105-2; fib Bulletin 66. Volume 2, pp. 370, ISBN 978-2-88394-106-9.
Nitschke A. G. and Winterberg R. (2016), Performance of macro-synthetic fiber reinforced tunnel linings. In: Proceedings of the World Tunnel Congress 2016, San Francisco (U.S.A.), 22-28 April, 2016, full-paper available on usb-stick, 10 p.
Rijke, Q.C. de (2006), Innovation of stress and damage reduction in bored tunnels during construction based on a shield equilibrium model, Graduate Thesis, Utrecht, Delft University of Technology and Holland Railconsult.
Rots J.G. (1988), Computational modeling of concrete fracture, Ph. D Thesis, Delft University of Technology, The Netherlands, pp. 132.
Selby R.G. and Vecchio F.J. (1993), Three dimensional constitutive relations for reinforced concrete, Univ. Toronto, Civil. Eng., Toronto, Canada.
Thorenfeldt E., Tomaszewicz A. and Jensen J. J. (1987), Mechanical properties of highstrength concrete and applications in design. In Proc. Symp. Utilization of High-Strength Concrete, Stavanger, Norway.
Tiberti G., Conforti A. and Plizzari G.A. (2015), Precast segments under TBM hydraulic jacks: Experimental investigation on the local splitting behavior, Tunnelling and Underground Space Technology, Vol. 50, August 2015, pp. 438-450, doi: http://dx.doi.org/10.1016/j.tust.2015.08.013.
Trabucchi I. (2015), Studio numerico di rivestimenti per gallerie realizzati in conci prefabbricati, Master Thesis, University of Brescia, pp. 250.
Trabucchi I., Conforti A., Tiberti G., Mudadu A and Plizzari G.A. (2019), Flexural behavior of precast tunnel segments reinforced by macro-synthetic fibers. In: Proceedings of the World Tunnel Congress 2019, Naples (Italy), 03-09 May, p. 9