Title: SP-334: Sustainable Concrete with Beneficial Byproducts

Author(s): Moncef L. Nehdi

Publication: Symposium Paper

Volume: 334

Issue:

Appears on pages(s): 152

Keywords: SP334

DOI: 10.14359/51721381

Date: 10/9/2019

Abstract:
To improve the eco-efficiency and sustainability of concrete, the cement and concrete industry can exploit many byproducts in applications that could, in some cases, outperform conventional materials made with traditional ingredients. This Special Publication of the American Concrete Institute Committee 555 (Concrete with Recycled Materials) is a contribution towards improving the sustainability of concrete via using recycled materials, such as scrap tire rubber and tire steel wire fiber, GFRP waste, fluff, reclaimed asphalt pavements, recycled latex paint, and recycled concrete aggregate. Advancing knowledge in this area should introduce the use of recycled materials in concrete for applications never considered before, while achieving desirable performance criteria economically, without compromising the quality and long-term performance of the concrete civil infrastructure.




  

Edit Module Settings to define Page Content Reviewer