Title:
ACI Reference Specifications
Author(s):
Bruce A. Suprenant
Publication:
Concrete International
Volume:
41
Issue:
10
Appears on pages(s):
42-48
Keywords:
requirement, checklist, specifier, project
DOI:
Date:
10/1/2019
Abstract:
A specification is a standard that establishes uniform criteria for a building product, assembly, technology, or project. Reference specifications can be important resources for code officials and specifiers creating contract documents. Citing an ACI reference specification in project specifications improves the quality of contract documents by providing an industry consensus standard that establishes uniform criteria for concrete construction.