Title:
Strength Recovery Through Nanosilica Coated Polypropylene Fiber Reinforcement
Author(s):
Su-Jin Lee, Shiho Kawashima, and Jong-Pil Won
Publication:
Symposium Paper
Volume:
335
Issue:
Appears on pages(s):
63-82
Keywords:
fiber reinforced; nano silica; polypropylene fiber; self-healing; sol-gel; strength
DOI:
10.14359/51720216
Date:
9/20/2019
Abstract:
In this study, nanosilica was applied to the surface of polypropylene (PP) fibers to introduce self-healing abilities when incorporated into cement-composites. When the fiber is at the site of a crack, the nanosilica can form additional hydration products through pozzolanic reaction to effectively seal the crack. Nanosilica was synthesized onto the fibers through a sol-gel process. Then the fibers were dried at room temperature or 50°C (122°F) to remove the excess solution and adhere the nanosilica particles onto the fiber surface. The existence of nanosilica was confirmed by observing the mass change before and after the sol-gel process, water absorption, soluble matter loss and microscopy. The self-healing performance of cement-composites reinforced with treated and untreated macro and micro PP fibers at dosages of 1.8kg/m3 (3.0lb/yd3) and 0.9kg/m3 (1.5lb/yd3), respectively, were evaluated through flexural strength testing according to ASTM C348. To evaluate strength recovery, samples were loaded to 60% of the peak load to induce cracking. The cracked specimens were cured for 28 days under laboratory conditions to undergo self-healing. A significant recovery in flexural strength (112.8%) was observed by using nanosilica treated micro PP fibers dried at room temperature.
Related References:
1. Mehta, P. K.; and Monteiro, P. J. M., “Concrete: Microstructure, Properties, and Materials,” 3rd edition, McGraw-Hill, 2006, pp. 21-84.
2. Hewlett, P. C., ed., “Lea's chemistry of cement and concrete,” 4th edition, Elsevier Ltd., 1998, pp.241-289.
3. Papatznni, S.; Paine, K.; and Calcabria-Holley, J., “Strength and microstructure of colloidal nanosilica enhanced cement pastes,” Cement and its Applications, V. 4, 2014, pp.80-85.
4. Shah, S. P.; Hou, P.; and Konsta-Gdoutos, M. S., “Nano-modification of cementitious material: toward a stronger and durable concrete,” Journal of Sustainable Cement-Based Materials, V. 5, No. 1-2, 2015, pp. 248-271.
5. Qing, Y.; Zenan, Z.; Deyu, K.; and Rongshen, C., “Influence of nano-SiO2 addition on properties of hardened cement paste as compared with silica fume,” Construction and Building Materials, V. 21, 2007, pp. 539-545.
6. Santos, S. F.; Rodrigues, J., A.; Tonoli, G. H. D.; Almeida, A. E. F. S.; and Savastano Jr, H., “Potential use of colloidal silica in cement based composites: Evaluation of the mechanical properties,” Key Engineering Materials, V. 517, 2012, pp. 389-391.
7. Jo, B.; Kim C.; and Lim, J., “Characteristics of cement mortar with nano-SiO2 particles,” ACI Materials Journal, V. 104, No. 4, 2007, pp. 404-407.
8. Bolhassani, M.; and Samani, M., “Effect of type, size, and dosage of nanosilica and microsilica on properties if cement paste and mortar,” ACI materials Journal, V. 112, No. 2, 2015, pp. 259-266.
9. Lu, C.; Li, S.; Lei, L; Wang, W.; Tao, F.; and Feng, L., “Bending strength properties of cement modified with nano-materials,” Electronic journal of geotechnical engineering, V. 20, 2015, pp. 3647-3654.
10. Thomas, J. J.; Jennings, H. M.; and Chen, J. J., “Influence of nucleation seeding on the hydration mechanisms of tricalcium silicate and cement,” The Journal of Physical Chemistry, V. 113, No. 11, 2009, pp. 4327-4334.
11. Land, G.; Stephan, D., “The influence of nanosilica on the hydration of ordinary Portland cement,” Journal of Material Science, V.47, 2012, pp. 1011-1017.
12. De Rooij, M.; Van Tittelboom, K.; De Belie, N.; and Erick, S., ed., “Self-healing phenomena in cementbased materials: State-of-the-Art Report of RILEM Technical Committee 221-SHC,” Springer, 2013, pp. 1-17, 65-214.
13. Hearn, N., “Self-sealing, autogenous healing and continued hydration: What is the difference?,” Material and Structures, V. 31, 1998, pp. 563-567.
14. Suleiman, A. R.; and Nehdi, M. L., “Effect of environmental exposure on autogenous self-healing of cracked cement-based materials,” Cement and Concrete Research, V. 111, 2018, pp. 197-208.
15. Tan, N. P. B.; Keung, L. H.; Choi, W. H.; Lam, W. C.; an Leung H. N., “Silica-based self-healing microcapsules for self-healing for self-repair in concrete,” Journal of Applied Polymer Science, V. 133, 2016, pp. 43090(1-12).
16. Shamaran, M.; Yıldırım, G.; Aras, G. H.; Keskin, S. B.; Keskin, Ő. K.; and Lachemi, M., “Self-healing of cementitious composites to reduce high CO2 emissions,” ACI Materials Journal, V. 114, No. 1, 2017, pp.93-104.
17. Wu, M.; Johannesson, B.; and Geiker, M., “A review: Self-healing in cementitious materials and engineered cementitious composite as a self-healing material,” Construction and Building Materials, V. 28, 2012, pp. 571-583.
18. Ferrara, L.; Ferreira, S. R.; Krelani, V.; Silvia, F.; and Toledo Filho, R. D., “Effect of natural fibres on the self-healing capacity of high performance fibre reinforced cementitious composite,” SHCC3-3rd International RILEM Conference on Strain Hardening Cementitious Composite, 2014, pp. 9-16.
19. Lee, M. W.; An, S.; Jo, H. S.; Yoon, S. S.; and Yarin A. L., “Self-healing nanofiber-reinforced polymer composites: 1. Tensile testing and recovery of mechanical properties,” ACS Applied Materials & Interfaces, V. 7, No. 35, 2015, pp. 19546-19554.
20. Homma, D.; Mihashi, H.; and Nishiwaki, T., “Self-healing capability of fibre reinforced cementitious composites,” Journal of Advanced Concrete Technology, V. 7, No. 2, 2009, pp. 217-228.
21. Herbert, E. N.; and Li, V. C., “Self-healing of microcracks in engineered cementitious composites (ECC) under a natural environment,” Materials, V. 6, No. 7, 2013, pp. 2831-2845.
22. Cuenca, E.; and Ferrara, L., “Self-healing capacity of fiber-reinforced cementitious composites: State of the art and perspective,” KSCE Journal of Civil Engineering, V. 21, No. 7, 2017, pp. 2777-2789.
23. Sofia, A., “Self-healing in ECC materials with high content of different micro-fibres and micro-particles,” MSc Thesis, Delft University of Technology, 2009.
24. Lee, S. J.; Kawashima, S.; Kim, K. J.; Woo, S. K.; and Won, J. P., “Interfacial properties of nanosilicatreated structural polymer fibres in cement matrix composites,” Composite Structures, V.202, 2018, pp.465-472.
25. Sobolev, K., “Nanotechnology and nanoengineering of construction materials,” Nanotechnology in construction, Sobolev K.; and Shah, S. P., ed., Springer, 2015, pp. 3-13.
26. Milea, C. A.; Bogatu, C.; and Duţă, A., “The influence of parameters in silica sol-gel process,” Bulletin of the Transilvania University of Braşov, V. 4, No. 53, 2011, pp. 59-66.
27. Shakmenko, G.; Juhnevica, I.; and Korjakins, A., “Influenc of sol-gel nanosilica on hardening process and physically-mechanical properties of cement paste,” Procedia Engineering, V. 57, 2013, pp. 1031-1021.
28. Arai, Y.; Segawa, H.; Yoshida, K., “Synthesis of nano silica particles for polishing prepared by sol-gel method,” Journal of Sol-Gel Science and Technology, V. 32, 2004, pp. 79-83.
29. Azlina, H. N.; Hasnidawani, J. N.; Norita, H.; and Surip, S. N., “Synthesis of SiO2 Nanostructures using solgel method,” Acta Physica Polonica A, V. 129, No. 4, 2016, pp. 842-844.
30. Buckley, A. M.; and Greenblatt, M., “The sol-gel preparation of silica gels,” Journal of Chemical Education, V. 71, No. 7, 1994, pp. 599-602.
31. Flores-Vivián, I.; and Sobolev, K., 2015, “The effect of nano-SiO2 on cement hydration,” Nanotechnology in construction, Sobolev K.; and Shah, S. P., ed., Springer, 2015, pp. 167-172.
32. Coppola, B.; Di Maio, L.; Scarfato, P.; and Incarnato, L., “Use of polypropylene fibers coated with nanosilica particles into a cementitious mortar,” AIP Conference Proceedings, V. 1695, No. 1, 2015, pp. 020056(1-9).
33. Yang, Z.; Liu, J.; Liu, J.; Li C.; and Zhou, H., “Silica modified synthetic fiber for improving interface property in FRCC,” 8th RILEM International Symposium on Fiber Reinforced Concrete: challenges and opportunities (BEFIB2012), 2012, pp. 347-357.
34. Di Maida, P.; Radi, E.; Scianclapore, C.; and Bondioli, F., “Pullout behavior of polypropylene macrosynthetic fibers treated with nano-silica,” Construction and Building Materials, V. 82, 2015, pp. 39-44.
35. Raabe, J.; dos Santos, L. P.; Del Menezzi, C. H. S.; amd Tonoli, G. H. E., “Effect of nano-silica deposition on cellulose fibers on the initial hydration of the Portland cement,” BioResources, V. 13, No. 2, 2018, pp. 3525-3544.
36. Hosseini, S. B.; Hedjazi, S.; Jamalirad, L.; and Sukhtesaraie, A., “Effect of the nano-SiO2 on physical and mechanical properties of fiber reinforced composites (FRCs),” Journal of the Indian Academy of Wood Science, V. 11, No. 2, 2014, pp. 116-121.
37. Ghazy, A.; Bassuoni, M. T.; Maguire, E.; and O’Loan, M., “Properties of Fiber-Reinforced Mortars Incorporating Nano-Silica,” Fibers, V. 4, No. 6, 2016, pp. 1-16.
38. Kong, D.; Du, X.; Wei, S.; Zhang, H.; Yang, Y.; and Shah, S. P. “Influence of nano-silica agglormeration on microstructure and properties of the hardened cement-based materials,” Construction and Building Materials, V. 37, 2012, pp. 707-715.
39. Herber, E.N.; and Li, V. C., “Self-healing of engineered cementitious composites in the natural environment,” Article in RILEM book series (High Performance Fiber Reinforced Cement Composite 6), 2012, pp.155-162
40. Yang, Y. Z.; Lepech, M.; Yang, E. H.; Li, V. C., “Autogenous healing of Engineered Cementitious Composites under wet-dry cycles,” Cement and Concrete Research, V. 39, 2009, pp. 382–390.
41. Berkowskia, P.; and Kosior-Kazberukb, M., “Effect of fiber on the concrete resistance to surface scaling due to cyclic freezing and thawing,” Procedia Engineering, V. 111, 2015, pp. 121-127.
42. Selvi1, M. T.; and Thandavamoorthy, T. S., “Studies on the Properties of Steel and Polypropylene Fibre Reinforced Concrete without any Admixture,” International Journal of Engineering and Innovative Technology, V. 3, No. 1, 2008, pp. 411-416.
43. Smirnova, O. M.; Shubin, A. A.; and Potseshkovskaya, I. V., “Strength and deformability properties of polyolefin macrofibers reinforced concrete,” International Journal of Applied Engineering Research, V. 12, No. 20, 2017, pp. 9397-9404.
44. Biricik, H.; and Sarier, N., “Comparative study of the characteristics of nano silica-, silica fume- and fly ashincorporated cement mortars,” Materials Research, V. 17, No. 3, 2014, pp. 570-582.
45. Quercia, G.; Lazaro, A.; Geus, J. W.; and Brouwers, H. J. H., “Characterization of morphology and texture of several amorphous nano-silica particles used in concrete,” Cement and Concrete Composites, V. 44, 2013, pp. 77-92.
46. Belkowitz, J. S.; Belkowitz, W. L. B.; Nawrocki, K.; and Fisher, F. T., “The impact of nano silica size and surface area in concrete properties,” ACI Material Journal, V. 112, No. 3, 2015, pp. 419-428.
47. Rahman, I. A.; and Padavetta, V., “Synthesis of silica nanoparticles by sol-gel: size-dependent properties, surface modification, and applications in silica-polymer nanocomposites-A review,” Journal of Nanomaterials, V. 2012, No. 8, 2012, pp. 132424(1-15).
48. Sun, X.; Wu, Q.; Zhang, J.; Qing, Y.; Wu, Y.; Lee, S., “Rheology, curing temperature and mechanical performance of oil well cement: Combined effect of cellulose nanofibers and graphene nano-platelets,” Materials & Design, V. 114, 2017, pp. 92-101.
49. Deboucha, W.; Leklou, N.; Khelidj, A.; Oudjit, M. N., “Hydration development of mineral additives blended cement using thermogravimeric analysis (TGA): Methodology of calculating the degree of hydration,” Construction and Building Materials, V. 146, 2017, pp. 687-701.
50. Rodriguez, E. T.; Garbev, K.; Merz, D.; Black, L.; and Richardson, I. G., “Thermal stability of C-S-H phases and applicability of Richardson and Groves’ and Richardson C-(A)-S-H(I) models to synthetic C-S-H,” Cement and Concrete Research, V. 93, 2017, pp. 45-56.
51. Collier, N. C., “Transition and decomposition temperatures of cement phases-A collection of thermal analysis data,” Ceramicc-Silikáty, V. 60, No, 4, 2016. pp. 338-434.
52. Zhang, Q.; and Ye, Q., “Dehydration kinetics of Portland cement paste at high temperature,” Journal of Thermal Analysis Calorimetry, V. 110, 2012, pp. 153-158.
53. Rupasinghe, M.; San Nicolas, R.; Mendis, P.; and Sofi, M., “Analysing the pozzolanic reactivity of nanosilica in cement paste,” Proceeding of 23rd Australasian Conference on the Mechanics of Structures and Materials (ACMSM23), 2014, pp. 131-136.