Abstract:
A total of five full-scale interior slab-column connections were tested under concentric monotonically increased loading. The slabs were 10 ft (3050 mm) square and 10 in. (254 mm) thick, and columns were 12 x 12 in. (305 x 305 mm). The specimens were built with Grade 60 reinforcement and 4000 psi (27.6 MPa) normal-weight concrete. Slab flexural tension reinforcement ratios were 0.87% in three specimens and 1.25% in the other two. One specimen with a slab reinforcement ratio of 0.87% was built without shear reinforcement. The other specimens were reinforced with headed shear studs. The studs were placed in either a radial or an orthogonal layout. Test results show that shear strength equations in the ACI Building Code overestimated the strength of the slab-column connections with a 0.87% slab flexural reinforcement ratio. Also, significant differences in failure mode were observed between slab-column connections with shear studs arranged in a radial layout and those with an orthogonal stud arrangement. Recommendations to improve shear strength of slab-column connections are presented.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer