Novel Admixtures to Reduce the Stickiness of Low W/C Concretes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Novel Admixtures to Reduce the Stickiness of Low W/C Concretes

Author(s): Manuel Ilg and Johann Plank

Publication: Symposium Paper

Volume: 329

Issue:

Appears on pages(s): 77-88

Keywords: concrete; stickiness; superplasticizer; non-ionic co-dispersant; polycarboxylate; flow properties; V-funnel; self-compacting concrete

DOI: 10.14359/51711205

Date: 9/26/2018

Abstract:
Concretes formulated at low water-cement ratios exhibit good material properties. Nevertheless, such concretes exhibit a honey-like consistency with a low speed of flow (“creeping behavior”) which is highly undesirable. In this paper it is shown that non-ionic small molecules can help to improve the fluidity at low water-cement ratios significantly and eliminate the “stickiness” when combined with ordinary PCE superplasticizers. For this purpose, different non-ionic glycol derivatives were screened via mini-slump testing. It was found that especially less polar species behave as very powerful co-dispersants. To gain a more profound understanding of the working mechanism, heat flow calorimetry was carried out. Additionally, concrete lab tests were performed to ascertain the impact of the non-ionic molecules on the V-funnel empty time of SCCs. Based on adsorption measurements it is inferred that the co-dispersants act as osmotic spacers which keep the cement particles apart and prevent them from agglomeration.

Related References:

1. Ramachandran, V. S.; Malhotra, V. M.; Jolicoeur, C.; and Spiratos, N., “Superplasticizers: Properties and applications in concrete”, CANMET, Ottawa, Canada, 1998.

2. Spiratos, N., Page, M., Mailvaganam, N. P., Malhotra, V. M., Jolicoeur, C., “Superplasticizers for Concrete: Fundamentals, Technology, and Practice”, Supplementary Cementing Materials for Sustainable Development, Ottawa, Canada, 2003.

3. Äitcin, P.-C., and Flatt, R., “Science and Technology of Concrete Admixtures (1st Edition)”, Woodhead Publishing, 2016.

4. Plank, J., “Concrete admixtures – Current status and perspectives for the future”, in: A. Badr, C. Fentiman, M. Grantham, R. Mangabhai, eds., “Concrete for the modern age – Developments in Materials and Process”, 2017, pp. 15 – 31.

5. Liu, J.; Wang, K.; Zhang, Q.; Han, F.; Sha, J.; and Liu, J., “Influence of superplasticizer dosage on the viscosity of cement paste with low water-binder ratio,” Construction & Building Materials, V. 149, 2017, pp. 359-366. doi: 10.1016/j.conbuildmat.2017.05.145

6. Lange, A., and Plank, P., “Optimization of comb-shaped polycarboxylate cement dispersants to achieve fast-flowing mortar and concrete,” Journal of Applied Polymer Science, V. 132, No. 37, 2015, p. 42529 doi: 10.1002/app.42529

7. Lange, A.; Hirata, T.; and Plank, J., “Influence of the HLB value of polycarboxylate superplasticizers on the flow behavior of mortar and concrete,” Cement and Concrete Research, V. 60, 2014, pp. 45-50. doi: 10.1016/j.cemconres.2014.02.011

8. Schmidt, W.; Brouwers, J.; Kühne, H. C.; and Meng, B., “Effects of superplasticizer and viscosity-modifying agent on fresh concrete performance of SCC at varied ambient temperatures, design, production and placement of self-consolidating concrete,” RILEM Bookseries, V. 1, 2010, pp. 65-77.

9. Ushiro, M.; Atarashi, D.; Kawakami, H.; and Sakai, E., “The effect of superplasticizer present in pore solution on flowability of low water-to-powder cement paste,” Cement Science and Concrete Technology, V. 67, No. 1, 2013, pp. 102-107. doi: 10.14250/cement.67.102

10. Lange, A.; Hirata, T.; and Plank, J., “The role of non-adsorbed PCE molecules in cement dispersion: experimental evidence for a new dispersion mechanism“, in: V. M. Malhotra, ed., Proceedings of the 10th CANMET/ACI Conference on Superplasticizers and Other Chemical Admixtures in Concrete, Prague (Czech Republic), 2012, SP-288.29, pp. 423 – 434.

11. Shui, L.; Sun, Z.; Yang, H.; Yang, X.; Ji, Y.; and Luo, Q., “Experimental evidence for a possible dispersion mechanism of polycarboxylate-type superplasticizers,” Advances in Cement Research, V. 28, No. 5, 2016, pp. 287-297. doi: 10.1680/jadcr.15.00070

12. Sakai, E.; Kakinuma, Y.; Yamamoto, K.; and Daimon, M., “Relation between the shape of silica fume and the fluidity of cement paste at low water to powder ratio,” Journal of Advanced Concrete Technology, V. 7, No. 1, 2009, pp. 13-20. doi: 10.3151/jact.7.13

13. Lange, A., and Plank, J., “Contribution of non-adsorbing polymers to cement dispersion,” Cement and Concrete Research, V. 79, 2016, pp. 131-136. doi: 10.1016/j.cemconres.2015.09.003

14. DIN 1164-10:2013-03 Special cement – Part 10: Composition, requirements and conformity evaluation for cement with low effective alkali content.

15. DIN EN 12350-8:2010-12 Testing fresh concrete – Part 8: Self compacting concrete – Slump flow test.

16. DIN EN 12350-9:2010-12 Testing fresh concrete – Part 9: Self-compacting concrete – V-funnel test.

17. Jakubekova, D.; Stibrany, P.; and Frtalova, D., “Investigation of the effects of diethylene glycol on the hydration of C3S and C3A pastes,” Journal of Thermal Analysis, V. 33, No. 3, 1988, pp. 651-659. doi: 10.1007/BF02138569