Title:
The Use of Vanadium Production Waste to Produce Alumina Cement
Author(s):
Kouznetsova T.V., Burlov I.Y., and Krivoborodov Y.R.
Publication:
Symposium Paper
Volume:
326
Issue:
Appears on pages(s):
47.1-47.6
Keywords:
calcium aluminates; cement; clinker; hydration; strength; solid solutions; waste
DOI:
10.14359/51711029
Date:
8/10/2018
Abstract:
The paper deals with the usage of slag waste from production of ferroalloys containing calcium and aluminum oxides, and also vanadium oxides as impurities. It is established that vanadium in small quantities at the synthesis of CA and CA2 forms with them solid solutions and increases their hydration activity. The optimum amount of vanadium oxide introduced into the composition of the initial raw mix is 3% wt. The carried out study showed that properties of alumina cement with a small quantity of V2O5 is useful. Hydration activity of alumina cement increases especially at early period of its hydration. Exceeding this value (more than 3%wt in row mix) leads the formation of CaO∙V2O5 along with calcium aluminates. But this compound is characterized by very low hydration activity. Therefore cement strength reduces.
Related References:
1. Midgley H.G., Ryder J.F. “The relationship between mineral composition and strength development of high alumina cement” Cem.Concr.Res., ?7, 1977, pp.669-672.
2. Toropov N.A. “Cement Chemistry”, Promstrojizdat, Leningrad, 1976, 156 pp.
3. Chatterji S., Jeffery D.W.” Microstructure of set high-alumina cement paste”, Trans. of British Ceram. Soc. ?5, 1968, pp.171-183.
4. Sawkow J.” Wysokoogniotrwale cement glinowe”. Cement- Wapno-Gips, v.31, ? 12,1978, pp.348 – 356.
5. Kurdowski W., George C.M., Sorentino F.P. “Special cements”, Proceeding of 8th ICCC, Rio de Janeiro, Brasil, 1986, v.1, pp.292-318.
6. Kouznetsova T.V. “Alumina and sulphoaluminate cements”, Strojizdat, ?oscow, 1986, 209 pp.
7. Kouznetsova T.V., Tanabep N. “Alumina cement”, Strojizdat, Moscow, 1988, 272 pp.
8. Krivoborodov Y.R., Boyko A.A.” Influence of mineral additions on hydration of alumina cement”, Technique and technology of silicates, v.18, ?4,2011, pp. 12-15.
9. Maki I. Relationship of processing parameters to clinker properties, Proceeding of 8th ICCC, Rio de Janeiro, Brasil, 1986, v.1, pp.35-47.
10. Osokin A.P.,Krivoborodov Y.R, Potapova E.N. “Modified Portland cement”, Strojizdat, Moscow, 1993, 328 pp.
11. Boikova A.I. “Solid solution of cement minerals”, Nauka, Leningrad, 1974, 99 pp.
12. ?urdowski W. “Cement and Concrete Chemistry” SPC, Krakow, 2010, 728 pp.
13. Taylor H.F.W. “Cement Chemistry”, Academic Press, London, 1990,475 pp.
14. Butt Y.M., Timashev V.V.” Portland Cement”, Strojizdat, Moscow,1974, 326 pp.
15. Kouznetsova T.V., Samchenko S.V.” Microscopy of materials of cement manufacture”, Public Centre MIKHSM, Moscow, 2007, 301 pp.