International Concrete Abstracts Portal

  


Title: Shear Behavior of Reinforced Concrete Beams made with Recycled Concrete Aggregates

Author(s): Nariman Khalil, Chelsea Tamer, and Fidel Abdo

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 44.1-44.10

Keywords: shear strength; recycled aggregate concrete; mechanical properties

DOI: 10.14359/51711026

Date: 8/10/2018

Abstract:
This paper presents a study into the shear behavior of reinforced concrete beams made with Recycled Concrete Aggregates (RCA). Three beams were cast. The first beam was made entirely with natural coarse aggregates to serve as control beam. The second beam was made with 50% replacement ratio of coarse aggregates and the third beam was made with 100% recycled concrete aggregates. The replacement was done by volume method. Replacement of sand was not considered. All beams had 150 x 300 mm cross section and were 3 m long. The reinforcement ratio was constant at ρ=1.04% with constant shear span a/d=3.5. The beams were subjected to four-point loading test. Twelve control specimens were cast with each beam to study the mechanical properties of the three concrete mixes designed. Beams’ deflection, crack patterns, yielding, ultimate shear capacity, and failure modes are all observed and analyzed. Results suggest no significant changes in the shear behavior as the replacement ratio of coarse aggregates increases. ACI Code provisions for predicting the concrete shear capacity are applicable to reinforced concrete beams made with recycled aggregates. This project is part of an ongoing research on the effect of the all parameters that affect the shear capacity of reinforced concrete beams.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.