Title:
Thermal Curing and Environmental Impact of Alkali-Activated Cementitious Materials
Author(s):
Elien Dejager, Steffen Grünewald, and Geert De Schutter
Publication:
Symposium Paper
Volume:
326
Issue:
Appears on pages(s):
21.1-21.10
Keywords:
alkali-activated materials; CO2-emissions; mix design; strength development; thermal curing
DOI:
10.14359/51711003
Date:
8/10/2018
Abstract:
During the production of ordinary Portland cement (OPC) clinker a lot of carbon dioxide (CO2) is emitted. To improve the sustainability of concrete production, many studies were carried out to evaluate alternative binders for OPC. The use of alkali-activated cementitious materials (AAMs) reduces the amount of Portland cement clinker and a larger volume of industrial by-products such as fly ash (FA) and blast furnace slag (BFS) can be applied. The combination of an aluminosilicate precursor and an alkali activator is characterised by a slower early age strength development compared to OPC. Thermal curing of the concrete is a successful technique to overcome this drawback. Although, thermal curing promotes the early age strength development of OPC-based concrete, the strength at 28 days often is relatively lower. In terms of environmental impact of AAMs, a significant reduction in production-related CO2-emissions is possible by replacing OPC by FA and/or BFS. With a relatively small activator dosage, it was found that the CO2-emissions can be decreased by up to 85% for AAMs compared to OPC-based mixtures. In this research, the effect of the mix design and curing temperature on the early age strength development and the environmental impact of AAMs was investigated.
Related References:
1. British Standard Institution (BSI), “Construction materials - Alkali-activated cementitious material and concrete”, Specification PAS 8820:2016, 2016, BSI Standards Limited.
2. Bruin, M, “Alternatieve bindmiddelen, what’s new?”, In: Dag van de Betontechnologie (p. 27). ENCI HeidelbergCement Group. Retrieved from http://www.joostdevree.nl/bouwkunde2/jpgb/bindmiddel_11_ alternatieve_bindmiddelen_enci_marcel_bruin_2015.pdf, 2015.
3. VWR, “Natriumhydroxide - Product details”, Retrieved November 20, 2016, from https://be.vwr.com/store/search/searchResultList.jsp;jsessionid=SgstQQBWSKTsV3Cy7Q1IMuai.estore8b?_dyncharset=UTF-8&_dynSessConf=7112902068576499559&keyword=28240.292&search.x=foo&%252Fvwr% 252Fsearch%252FSearchFormHandler.searchRequest.searchOperator=and&_D%253A%25, 2016a.
4. VWR, “Natriumsilicaat waterige oplossing - Product details”, Retrieved November 20, 2016, from https://be.vwr.com/store/catalog/product.jsp?catalog_number=28079.320, 2016b.
5. Holcim, “CEM I 52.5 R HES”, Sint-Pieters-Leeuw, 2006.
6. Onghena, S., “Strength development of concrete in prefabricated elements: balancing production requirements and ecological impact”, 2015, Ghent University.
7. NBN EN 196-1, “NBN EN 196-1 - Beproevingsmethoden voor cement - Deel 1: Bepaling van de sterkte”, Brussel: Bureau voor Normalisatie, 2005.
8. NBN EN 12350-2, “NBN EN 12350-2 - Beproeving van betonspecie - Deel 2: Zetmaat”, Brussel: Bureau voor Normalisatie, 2009.
9. NBN EN 1015-3, “NBN EN 1015-3 - Proeven voor metselmortel - Deel 3: Bepalen van consistentie van verse mortel (met de schoktafel)”, Brussel: Bureau voor Normalisatie, 1999.
10. NBN EN 196-9, “NBN EN 196-9: Beproevingsmethoden van cement (Deel 9: Hydratatiewarmte - Semi-adiabatische methode”, Brussel: Bureau voor Normalisatie, 2010.
11. Pacheco-Torgal, F., Labrincha, J. A., Leonelli, C., Palomo, A. and Chindaprasirt, P., “Handbook of Alkali-acitvated Cements, Mortars and Concretes”, (Elsevier Ltd., Ed.), Part Two The properties of alkali-activated cement, mortar and concrete binders Woodhead Publishing, ISBN 978-0-85709-028-7, ISBN 978-1-84569-349-7, ISBN 978-0-85709-424-7, 2015.
12. Taerwe, L. and De Schutter, G., “Betontechnologie”, Ghent University, 2006.
13. Gruyaert, E., Effect of Blast-Furnace Slag as Cement Replacement on Hydration, Microstructure, Strength and Durability of Concrete, Ghent University, 2010.
14. SBR CUR net, “CUR-Ontwerptool - Groen beton”, Retrieved March 21, 2017, from
http://www.sbrcurnet.nl/producten/rekentools/cur-ontwerptool-groen-beton-1, 2017.