Abstract:
This session will highlight a diverse range of infrastructure project types on the U.S. West Coast and the innovative uses of precast concrete, cast-in-place concrete, and grout to solve complex engineering issues. Various applications of concrete pavements will also be discussed from both the client and designer perspective to understand the current serviceability challenges and advancements geared toward producing longer-lasting concrete pavements.