Title: ESTUDIO EXPERIMENTAL DE LAS PERDIDAS DE PRETENSADO POR ROZAMIENTO, DE TEN-

Author(s): MORERA J.M.

Publication: ACHE

Volume: 33

Issue: 143

Appears on pages(s): 12 -

Keywords:

DOI:

Date: 1/3/1982

Abstract: