Sectional ductility and redistribution of internal forces in statically indeterminate reinforced and prestressed concrete structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sectional ductility and redistribution of internal forces in statically indeterminate reinforced and prestressed concrete structures

Author(s): Marí Bernat, A.

Publication: ACHE

Volume: 38

Issue: 163

Appears on pages(s): 31 - 54

Keywords:

DOI:

Date: 1/3/1987

Abstract:
En primer lugar, se muestra la conveniencia de garantizar un mínimo de ductilidad en las secciones criticas de pórticos y vigas 'continuas de hormigón armado, para evitar roturas localizadas bajo niveles de carga inferiores al de proyecto, mediante el am1lisis no lineal de dos ejemplos concretos. Tras plantear las relaciones analíticas entre los diversos parámetros que intervienen en el comportamiento seccional en rotura, se describe un procedimiento para el dimensionamiento de secciones rectangulares con un nivel de ductilidad prefijado. Por otra parte, se hace una revisión del tratamiento que diversas normativas dan al tema de las condiciones de ductilidad exigidas a las secciones criticas para garantizar un nivel de redistribución de esfuerzos, as} como para aceptar el análisis lineal elástico, estableciendo comparaciones y sugiriendo la modificación de la normativa española en relación con estos aspectos. Por último, se presentan algunos ejemplos de dimensionamiento de vigas para diversos niveles de redistribución, extrayendo conclusiones relativas a la economía y racionalidad de las soluciones presentadas.