Title:
The materials in the Eurocode 4
Author(s):
Valiente Cancho, A.; Navarro Ugena, C.
Publication:
ACHE
Volume:
43
Issue:
185
Appears on pages(s):
17 - 27
Keywords:
DOI:
Date:
1/8/1992
Abstract:
The behaviour of structural materials, as considered in EC4 for composite steel and concrete structuers, is analyzed in this work. The mechanical and thermomechanical models assumed by the eurocode for concrete and steel are reviewed, as well as the material properties ffrom which the models are cuantitatively characterized.