Title: Supression of several aligned pillar in a special structure at La Coruña

Author(s): González Serrano, A.

Publication: ACHE

Volume: 47

Issue: 200

Appears on pages(s): 73 - 78

Keywords:

DOI:

Date: 1/3/1996

Abstract:
This paper explains the method carried out to supress a line of pillars in a special structure with big loads.