Title: Modelling the Bond Fatigue Behavior of Concrete Beams Strengthened with Prestressed NSM CFRP Rods

Author(s): Noran Wahab, Timothy Topper, and Khaled A. Soudki

Publication: Symposium Paper

Volume: 322

Issue:

Appears on pages(s): 13.1-13.16

Keywords: bond, debonding, prestressed, fatigue load, NSM, shear stress, rod

DOI: 10.14359/51706964

Date: 6/18/2018

Abstract:
Near surface mounted (NSM) is a promising strengthening technique provided that the full bond between the strengthening material and the existing structure develops. Wahab et al. (2011 and 2012) tested reinforced concrete beams to asses the bond strength between the prestressed NSM carbon fibre reinforced polymers (CFRP) rods and the concrete. The beams were tested in four points bending under different fatigue load levels. Failure was by slipping between the CFRP rod and the epoxy that started at the support and traveled to the loading point as the number of cycles was increased. Modeling of the failure of the beams is presented in this paper. When the CFRP rod is prestressed, the shear stress is largest at the free end and decreases along the transfer length. The prestressing shear stresses are taken equal to the cracking shear stress under monotonic load for non-prestressed beams. During loading, following flexural cracking, debonding occurs at the loading point and progresses towards the supports as the load is cycled. The debonding is modeled as a crack growing at the interface between the CFRP rod and the epoxy. A bond stress versus slip model is proposed. It consists of an ascending branch representing the strains and stresses ahead of the crack tip and a descending branch representing the region behind the crack tip. The driving force for the crack is the shear stresses at the interface between the CFRP rod and the epoxy. The overlapping of the two shear stress distributions increases the shear stress near the end of the beam, which becomes the critical shear stress that causes failure. The failure shear stress at the end is higher than the prestressing shear stress and is estimated to be 25.5 MPa (3.698 ksi) for the spirally wound rods and 30.4 MPa (4.409 ksi) for the sand coated rods. The model also predicts the number of cycles and the forces in the CFRP rod at all locations in the shear span at the onset of failure with reasonable accuracy.

Related References:

1. Achintha P. M. M., and Burgoyne C. J. (2008). “Fracture Mechanics of Plate Debonding.” Journal of Composites for Construction, Volume 12, No. 4, pp. 396-404.

2. De Lorenzis L., Lundgren K., and Rizzo A. (2004). “Anchorage Length of Near Surface Mounted FRP Bars for Concrete Strengthening – Experimental Investigation and Numerical Modeling.” ACI Structural Journal, Volume 101, No. 2, pp. 269-278.

3. De Lorenzis L., and Nanni A. (2002). “Bond between NSM Fiber-Reinforced Polymer Rods and Concrete in Structural Strengthening.” ACI Structural Journal, Volume 99, No. 2, pp. 123-32.

4. De Lorenzis L., Rizzo A., and La Tegola A. A.(2002). “Modified Pull-out Test for Bond of Near-Surface Mounted FRP Rods in Concrete.” Composites-Part B: Engineering, Volume 33, No. 8, pp. 589–603.

5. Dowling N. (2006).“Mechanical Behavior of Materials”, Prentice Hall; 3rd edition.

6. Harries K.A., Richard M., and Kim Y. (2010). “Fatigue of CFRP Retrofitted Damaged Steel Beams.” Proceedings of the 2010 International Conference on Structural Faults and Repair, Engineering Technics Press, Edinburgh, United Kingdom.

7. Huang D., and Lyons J. (2007). “ Numerical Stress Analysis of the Bond between a Reinforced Concrete T-Beam and FRP Sheets.” Journal of Reinforced Plastics and Composites, Volume 26, No. 12, pp. 1225-1237.

8. Mazzotti C., Savoia M., and Ferracuti B. (2005).“FRP – Concrete Delamination Results Adopting Different Experimental Pure Shear Set Ups.”11th International Conference on Fracture, Curran Associates, New York, USA, pp. 1518-1523.

9. Oudah F., and El-Hacha R. (2012-a). ”Performance of RC Beams Strengthened Using Prestressed NSM-CFRP Strips Subjected to Fatigue Loading.” J. Compos. Constr., Volume16, No. 3, pp.300–307.

10. Oudah F., and El-Hacha R. (2012-b). “Fatigue behaviour of RC beams strengthened with prestressed NSM CFRP rods.“ Journal of Composite Structures, Volume 94, No.4, pp. 1333-1342.

11. Oudah F., and El-Hacha R. (2013). “Analytical fatigue prediction model of RC beams strengthened in flexure using prestressed FRP reinforcement.” Engineering Structures, Volume 46, pp. 173-183.

12. Omran H., and El-Hacha R. (2012).” Nonlinear 3D finite element modeling of RC beams strengthened with prestressed NSM-CFRP strips.” Construction and Building Materials, Volume 31, pp. 74-85.

13. The International Federation for Structural Concrete (FIB). (2000). “Bond of Reinforcement in Concrete.” Stateof-art report, International Federation for Structural Concrete, Lausanne, Switzerland.

14. Wahab N., Soudki K.A., and Topper T. (2008). "Bond of Carbon Fiber Reinforced Polymer Rods to Concrete in Near-Surface Mounted Application under Fatigue Loading." Proc. 2nd Canadian Conference on Effective Design

of Structures, McMaster University, Centre for Effective Design of Structures, Department of Civil Engineering, Hamilton, Ontario, Canada, pp.195-205.

15. Wahab N., Soudki K.A., and Topper T. (2012). ”Experimental Investigation of Bond Fatigue Behavior of Concrete Beams Strengthened with NSM Prestressed CFRP Rods.” J. Compos. Constr., Volume 16, No. 6, pp. 684–692.

16. Wahab N., Soudki K.A., and Topper T. (2011). ”Mechanics of Bond Fatigue Behavior of Concrete Beams Strengthened with NSM CFRP Rods.” J. Compos. Constr., Volume 15, No. 6, pp. 934–942.

17. Wahab N., Topper T., and Soudki KA. (2015). ” Modelling experimental bond fatigue failures of concrete beams strengthened with NSM CFRP rods.” Composites Part B: Engineering, Volume 70, No. 1, March 2015, pp. 113-121, ISSN 1359-8368, http://dx.doi.org/10.1016/j.compositesb.2014.10.040.