Title: ITG-10R: Practitioner's Guide for Alternative Cements

Author(s): ACI Innovation Task Group 10

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 14

Keywords: alkali-activated fly ash cement; alkali-activated glass cement; alkali-activated slag cement; alkali activation; alternative cements; calcium aluminate cement; calcium sulfoaluminate cement; carbonated calcium silicate cement; ITG; ITG10

DOI:

Date: 4/24/2018

Abstract:
As performance demands of concrete increase, and given recent initiatives to address the sustainability of construction, owners, architects, and engineers are actively seeking alternatives to portland cement for concrete. An alternative cement is intended to be a replacement for portland cement in some applications. In some cases, alternative cements may also be used in combination with portland or blended hydraulic cements. This document covers currently available and emerging alternative cements and is intended to provide information to help guide practitioners seeking to implement alternative cements.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer