International Concrete Abstracts Portal

  


Title: Out-of-Plane Reinforcement of Masonry Walls with Steel Reinforced Grout

Author(s): Stefano De Santis, Gianmarco de Felice

Publication: Symposium Paper

Volume: 324

Issue:

Appears on pages(s): 9.1-9.14

Keywords: masonry, out-of-plane, seismic retrofitting, shake table tests.

DOI: 10.14359/51702361

Date: 4/1/2018

Abstract:
A shake table investigation was carried out on a full-scale U-shaped masonry assemblage to study the effectiveness of Steel Reinforced Grout (SRG) for the improvement of the out-of-plane seismic capacity of masonry walls. Natural accelerograms were applied with increasing scale factor up to failure. A first session of tests was performed on the unreinforced specimen, that collapsed by out-of-plane overturning. Steel tie bars were then installed to prevent overturning. In this case, severe damage developed due to bending. Finally, the wall was retrofitted with horizontal strips of Ultra High Tensile Strength Steel cords, externally bonded to the masonry with lime based mortar, and steel connectors. SRG led to a significant improvement of the seismic capacity, strongly limited damage development, and entailed small modifications of the dynamic properties of the specimen. Since the reinforcement had a thickness of less than 10mm, it is suitable for applications within the plaster layer during the maintenance work of the façades without modifying their appearance.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer