Title: Vibration Characteristics of Micro-Engineered Crumb Rubber Concrete for Railway Sleeper Applications

Author(s): Ratthaphong Meesit, Sakdirat Kaewunruen

Publication: JCI

Volume: 15

Issue: 2

Appears on pages(s): 55 - 66

Keywords:

DOI: 10.3151/jact.15.55

Date: 1/1/2017

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  