Title:
Mechanical Behavior of Widening Prestressed Concrete Deck Slabs under Concentrated Load
Author(s):
Fakhruddin, Takuro Nakamura, Yuji Sato, Masahiko Yamada, Junichiro Niwa
Publication:
JCI
Volume:
15
Issue:
2
Appears on pages(s):
38 - 54
Keywords:
DOI:
10.3151/jact.15.38
Date:
1/1/2017
Abstract: